Detectability by X-ray micro computed tomography of fatigue initiating void defects in laser powder-bed additively manufactured Ti-6Al-4V coupons AITranslate

Defence Science Technology Group, Fishermans Bend; Air Force Research Laboratory;Defence Science Technology Group, Fishermans Bend;Defence Science Technology Group, Fishermans Bend;Defence Science Technology Group, Fishermans Bend;Defence Science Technology Group, Fishermans Bend
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Non-destructive inspection is important for the quality assurance of additively manufactured components. In this study, X-ray micro Computed Tomography (µCT) was assessed for its capabilities and limitations to detect fatigue-initiation porosities in Ti-6Al-4V additively manufactured coupons. Cylindrical coupons were built using laser powder-bed fusion (L-PBF) from three different vendors and four different L-PBF machines that utilized their default process parameters. Using OEM prescribed default process parameters, there was significant variability in the defect distribution between machine to machine and also coupon to coupon that was on the same build plate, primarily due the difference in the internal quality assurance procedures and scan strategies adopted by each vendor. The probability of detection for conventional µCT (cubic voxel size 17.77 µm) was investigated by comparing with what was detected using a Synchrotron Radiation Micro Computed Tomography (SRµCT) at cubic voxel size 5.91 µm. It was found that µCT’s detectability relative to SRµCT was approximately 90% for defect diameters of the circumscribed sphere of 230 µm and above and 100% for diameters of 340 µm and above (12–14 times the voxel size of the µCT scan). The type of defect was a key factor to the detectability of large sized defects (>200 µm in diameter) due to the flatness and elongated shape factors. Fatigue results showed the critical defect √Area at the surface was approximately 100 µm at 500 MPa stress level, where significant scatter in fatigue life was observed. Post-fatigue test fractography identified different types of fatigue initiating defects, of which a ‘flat’ lack-of-fusion type defect was undetectable by either µCT or SRµCT. This type of defect was extremely flat and occupied very little spatial resolution through the build direction which limited the detection by automated threshold-based defect detection algorithms.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.addma.2024.103986

Chinese Library Classification Number:

Citation Information:

Non-destructive inspection is important for the quality assurance of additively manufactured components. In this study, X-ray micro Computed Tomography (µCT) was assessed for its capabilities and limitations to detect fatigue-initiation porosities in Ti-6Al-4V additively manufactured coupons. Cylindrical coupons were built using laser powder-bed fusion (L-PBF) from three different vendors and four different L-PBF machines that utilized their default process parameters. Using OEM prescribed default process parameters, there was significant variability in the defect distribution between machine to machine and also coupon to coupon that was on the same build plate, primarily due the difference in the internal quality assurance procedures and scan strategies adopted by each vendor. The probability of detection for conventional µCT (cubic voxel size 17.77 µm) was investigated by comparing with what was detected using a Synchrotron Radiation Micro Computed Tomography (SRµCT) at cubic voxel size 5.91 µm. It was found that µCT’s detectability relative to SRµCT was approximately 90% for defect diameters of the circumscribed sphere of 230 µm and above and 100% for diameters of 340 µm and above (12–14 times the voxel size of the µCT scan). The type of defect was a key factor to the detectability of large sized defects (>200 µm in diameter) due to the flatness and elongated shape factors. Fatigue results showed the critical defect √Area at the surface was approximately 100 µm at 500 MPa stress level, where significant scatter in fatigue life was observed. Post-fatigue test fractography identified different types of fatigue initiating defects, of which a ‘flat’ lack-of-fusion type defect was undetectable by either µCT or SRµCT. This type of defect was extremely flat and occupied very little spatial resolution through the build direction which limited the detection by automated threshold-based defect detection algorithms.

quote

GB/T 7714-2015 [1] Stephen Sun, Jonathan D. Miller, Yi Rye Choi, et al. Additive Manufacturing, 2024(81). DOI:10.1016/j.addma.2024.103986.
MLA [1] Stephen Sun, et al., Additive Manufacturing, no. 81, 2024, https://doi.org/10.1016/j.addma.2024.103986.
APA [1] Stephen Sun, Jonathan D. Miller, Yi Rye Choi, Suzana Turk, Drew Donnelly, & Qianchu Liu. (2024). Additive Manufacturing(81). https://doi.org/10.1016/j.addma.2024.103986
IEEE [1] Stephen Sun, Jonathan D. Miller, Yi Rye Choi, Suzana Turk, Drew Donnelly, and Qianchu Liu, Additive Manufacturing, no. 81, 2024, doi: 10.1016/j.addma.2024.103986.