daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Light- and Temperature-Modulated Magneto-Transport in Organic–Inorganic Lead Halide Perovskites AITranslate

Molecular Imaging and Photonics, Department of Chemistry; Radboud University;Molecular Imaging and Photonics, Department of Chemistry;Molecular Imaging and Photonics, Department of Chemistry;Department of Molecular and Microbial Systems, KU Leuven;Molecular Imaging and Photonics, Department of Chemistry
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The optoelectronic properties and charge carrier dynamics in hybrid organic–inorganic perovskites under steady-state illumination are the key elements for understanding their high efficiency. We present temperature-dependent Hall and photoconductivity measurements down to a temperature of 4.2 K on single crystals of MAPbI3 and MAPbBr3 in magnetic fields up to 30 T and observed different transport regimes. For temperatures down to 25 K, charge transport is dominated by acoustic phonon scattering as inferred from the temperature dependence of both zero and high-field resistance. Below 25 K, transport is determined by thermally activated hopping of charge carriers reflected in a diverging zero-field resistance and a strong decrease in the carrier’s mobility and concentration. Our findings demonstrate the importance of performing experiments at low temperature to unravel the fundamental charge carrier dynamics and stimulate the need for a comprehensive theoretical model for perovskite-based devices.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.7b00941

Chinese Library Classification Number:

Citation Information:

The optoelectronic properties and charge carrier dynamics in hybrid organic–inorganic perovskites under steady-state illumination are the key elements for understanding their high efficiency. We present temperature-dependent Hall and photoconductivity measurements down to a temperature of 4.2 K on single crystals of MAPbI3 and MAPbBr3 in magnetic fields up to 30 T and observed different transport regimes. For temperatures down to 25 K, charge transport is dominated by acoustic phonon scattering as inferred from the temperature dependence of both zero and high-field resistance. Below 25 K, transport is determined by thermally activated hopping of charge carriers reflected in a diverging zero-field resistance and a strong decrease in the carrier’s mobility and concentration. Our findings demonstrate the importance of performing experiments at low temperature to unravel the fundamental charge carrier dynamics and stimulate the need for a comprehensive theoretical model for perovskite-based devices.

quote

GB/T 7714-2015 [1] Masoumeh Keshavarz, Steffen Wiedmann, Haifeng Yuan, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.7b00941.
MLA [1] Masoumeh Keshavarz, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.7b00941.