daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Rational Design of a Multifunctional Binder for High-Capacity Silicon-Based Anodes AITranslate

Oak Ridge National Laboratory; Oak Ridge National Laboratory; University of Tennessee; Oak Ridge National Laboratory; University of Tennessee; Argonne National Laboratory; Oak Ridge National Laboratory; Argonne National Laboratory; University of Tennessee; Oak Ridge National Laboratory; Oak Ridge National Laboratory
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Although several principles have been recognized to fabricate a nominal “better” binder, there continues to be a lack of a rational design and synthesis approach that would meet the robust criteria required for silicon (Si) anodes. Herein, we report a synthetic polymer binder, i.e., catechol-functionalized chitosan cross-linked by glutaraldehyde (CS-CG+GA), that serves dual functionalities: (a) wetness-resistant adhesion capability via catechol grafting and (b) mechanical robustness via in situ formation of a three-dimensional (3D) network. A SiNP-based anode with a designed functional polymer network (CS-CG10%+6%GA) exhibits a capacity retention of 91.5% after 100 cycles (2144 ± 14 mAh/g). Properties that are traditionally considered to be advantageous, including stronger adhesion strength and higher mechanical robustness, do not always improve the binder performance. A clear relationship between these properties and ultimate electrochemical performance is established by assessing the rheological behavior, mechanical property, adhesion force, peel stress, morphology evolution, and semiquantitative evaluation. This study provides a clear path for the rational design of high-performance functional polymer binders for not only Si-based electrodes but also other types of alloy and conversion-based electrodes.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b00815

Chinese Library Classification Number:

Citation Information:

Although several principles have been recognized to fabricate a nominal “better” binder, there continues to be a lack of a rational design and synthesis approach that would meet the robust criteria required for silicon (Si) anodes. Herein, we report a synthetic polymer binder, i.e., catechol-functionalized chitosan cross-linked by glutaraldehyde (CS-CG+GA), that serves dual functionalities: (a) wetness-resistant adhesion capability via catechol grafting and (b) mechanical robustness via in situ formation of a three-dimensional (3D) network. A SiNP-based anode with a designed functional polymer network (CS-CG10%+6%GA) exhibits a capacity retention of 91.5% after 100 cycles (2144 ± 14 mAh/g). Properties that are traditionally considered to be advantageous, including stronger adhesion strength and higher mechanical robustness, do not always improve the binder performance. A clear relationship between these properties and ultimate electrochemical performance is established by assessing the rheological behavior, mechanical property, adhesion force, peel stress, morphology evolution, and semiquantitative evaluation. This study provides a clear path for the rational design of high-performance functional polymer binders for not only Si-based electrodes but also other types of alloy and conversion-based electrodes.

quote

GB/T 7714-2015 [1] PengFei Cao, Guang Yang, Bingrui Li, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00815.
MLA [1] PengFei Cao, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00815.
APA [1] PengFei Cao, Guang Yang, Bingrui Li, Yiman Zhang, Sheng Zhao, Shuo Zhang, Andrew Erwin, Zhengcheng Zhang, Alexei P. Sokolov, Jagjit Nanda, & Tomonori Saito. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00815
IEEE [1] PengFei Cao, Guang Yang, Bingrui Li, Yiman Zhang, Sheng Zhao, Shuo Zhang, Andrew Erwin, Zhengcheng Zhang, Alexei P. Sokolov, Jagjit Nanda, and Tomonori Saito, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00815.