daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Identifying and Reducing Interfacial Losses to Enhance Color-Pure Electroluminescence in Blue-Emitting Perovskite Nanoplatelet Light-Emitting Diodes AITranslate

University of Cambridge; University of Cambridge; University of Cambridge; Nano-Institute Munich; Nicolaus Copernicus University; University of Cambridge; University of Cambridge; University of Cambridge; Nicolaus Copernicus University; Nano-Institute Munich; Nano-Institute Munich; University of Cambridge; University of Cambridge; Nano-Institute Munich; University of Cambridge
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Perovskite nanoplatelets (NPls) hold promise for light-emitting applications, having achieved photoluminescence quantum efficiencies approaching unity in the blue wavelength range, where other metal-halide perovskites have typically been ineffective. However, the external quantum efficiencies (EQEs) of blue-emitting NPl light-emitting diodes (LEDs) have reached only 0.12%. In this work, we show that NPl LEDs are primarily limited by a poor electronic interface between the emitter and hole injector. We show that the NPls have remarkably deep ionization potentials (≥6.5 eV), leading to large barriers for hole injection, as well as substantial nonradiative decay at the NPl/hole-injector interface. We find that an effective way to reduce these nonradiative losses is by using poly(triarylamine) interlayers, which lead to an increase in the EQE of the blue (464 nm emission wavelength) and sky-blue (489 nm emission wavelength) LEDs to 0.3% and 0.55%, respectively. Our work also identifies the key challenges for further efficiency increases.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b00571

Chinese Library Classification Number:

Citation Information:

Perovskite nanoplatelets (NPls) hold promise for light-emitting applications, having achieved photoluminescence quantum efficiencies approaching unity in the blue wavelength range, where other metal-halide perovskites have typically been ineffective. However, the external quantum efficiencies (EQEs) of blue-emitting NPl light-emitting diodes (LEDs) have reached only 0.12%. In this work, we show that NPl LEDs are primarily limited by a poor electronic interface between the emitter and hole injector. We show that the NPls have remarkably deep ionization potentials (≥6.5 eV), leading to large barriers for hole injection, as well as substantial nonradiative decay at the NPl/hole-injector interface. We find that an effective way to reduce these nonradiative losses is by using poly(triarylamine) interlayers, which lead to an increase in the EQE of the blue (464 nm emission wavelength) and sky-blue (489 nm emission wavelength) LEDs to 0.3% and 0.55%, respectively. Our work also identifies the key challenges for further efficiency increases.

quote

GB/T 7714-2015 [1] Robert L. Z. Hoye, MayLing Lai, Miguel Anaya, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00571.
MLA [1] Robert L. Z. Hoye, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00571.
APA [1] Robert L. Z. Hoye, MayLing Lai, Miguel Anaya, Yu Tong, Krzysztof Gałkowski, Tiarnan Doherty, Weiwei Li, Tahmida N. Huq, Sebastian Mackowski, Lakshminarayana Polavarapu, Jochen Feldmann, Judith L. MacManusDriscoll, Richard H. Friend, Alexander S. Urban, & Samuel D. Stranks. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00571
IEEE [1] Robert L. Z. Hoye, MayLing Lai, Miguel Anaya, Yu Tong, Krzysztof Gałkowski, Tiarnan Doherty, Weiwei Li, Tahmida N. Huq, Sebastian Mackowski, Lakshminarayana Polavarapu, Jochen Feldmann, Judith L. MacManusDriscoll, Richard H. Friend, Alexander S. Urban, and Samuel D. Stranks, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00571.