daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Influence of synthesis parameters on g-C3N4 polysulfides trapping: A systematic study AITranslate

Electrochemistry Group, Department of Applied Science and Technology (DISAT);YPF Tecnología S.A., Av. Del Petroleo s/n - (Entre 129 y 143);Electrochemistry Group, Department of Applied Science and Technology (DISAT);Electrochemistry Group, Department of Applied Science and Technology (DISAT); Universidad Nacional de Córdoba; Universidad Nacional de La Plata;Electrochemistry Group, Department of Applied Science and Technology (DISAT)
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Beyond Li-ion batteries, one of the most promising technology is the Lithium-Sulphur (Li-S) not only for its higher theoretical energy density (about 2600 Wh kg−1) but because sulfur is relatively inexpensive and non-toxic. However, the Li-S battery suffers from “shuttle effect” of polysulfides. Thus, restricting shuttling means increasing cell performance and durability. DFT calculations showed that graphitic carbon nitride (g-C3N4) exhibits strong interactions with Li2S (e.g. superior to graphene-like carbon) and acts as polysulfides trapping agent. In this work, the role of g-C3N4, synthetized from different precursor and at different polycondensation temperatures was systematically studied, using a double layer approach for the electrode preparation, which ensures direct interaction between g-C3N4 and soluble lithium-polysulfides. This systematic study confirms the importance of the morphological and superficial properties of the material. In particular, carbon nitride from urea precursor remarkably improves the performance of the sulphur cathode, increasing the specific capacity of the cell by 25% and improving its useful life over 500 cycles. According to the morphological characterization and the XPS analysis, benefits are achieved from polycondensation of urea at 550°C. The obtained g-C3N4 shows the highest proportion of -NH2 species on the surface, which favours the interaction with polysulfides. Graphical abstract Download : Download high-res image (186KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2021.101169

Chinese Library Classification Number:

Citation Information:

Beyond Li-ion batteries, one of the most promising technology is the Lithium-Sulphur (Li-S) not only for its higher theoretical energy density (about 2600 Wh kg−1) but because sulfur is relatively inexpensive and non-toxic. However, the Li-S battery suffers from “shuttle effect” of polysulfides. Thus, restricting shuttling means increasing cell performance and durability. DFT calculations showed that graphitic carbon nitride (g-C3N4) exhibits strong interactions with Li2S (e.g. superior to graphene-like carbon) and acts as polysulfides trapping agent. In this work, the role of g-C3N4, synthetized from different precursor and at different polycondensation temperatures was systematically studied, using a double layer approach for the electrode preparation, which ensures direct interaction between g-C3N4 and soluble lithium-polysulfides. This systematic study confirms the importance of the morphological and superficial properties of the material. In particular, carbon nitride from urea precursor remarkably improves the performance of the sulphur cathode, increasing the specific capacity of the cell by 25% and improving its useful life over 500 cycles. According to the morphological characterization and the XPS analysis, benefits are achieved from polycondensation of urea at 550°C. The obtained g-C3N4 shows the highest proportion of -NH2 species on the surface, which favours the interaction with polysulfides. Graphical abstract Download : Download high-res image (186KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Daniele Versaci, Melina Cozzarin, Julia Amici, et al. Applied Materials Today, 2021(25). DOI:10.1016/j.apmt.2021.101169.
MLA [1] Daniele Versaci, et al., Applied Materials Today, no. 25, 2021, https://doi.org/10.1016/j.apmt.2021.101169.
APA [1] Daniele Versaci, Melina Cozzarin, Julia Amici, Carlotta Francia, Ezequiel P.M. Leiva, Arnaldo Visintin, & Silvia Bodoardo. (2021). Applied Materials Today(25). https://doi.org/10.1016/j.apmt.2021.101169
IEEE [1] Daniele Versaci, Melina Cozzarin, Julia Amici, Carlotta Francia, Ezequiel P.M. Leiva, Arnaldo Visintin, and Silvia Bodoardo, Applied Materials Today, no. 25, 2021, doi: 10.1016/j.apmt.2021.101169.