Thermodynamic modeling and optimization of the Fe–Ni–Ti system AITranslate

Dept. Metaalkunde en Toegepaste Materiaalkunde (MTM), Faculty of Engineering Sciences;Dip. di Chimica e Chimica Industriale, Università di Genova;Calcule Thermodynamique, 3 rue de l’Avenir;Dept. Metaalkunde en Toegepaste Materiaalkunde (MTM), Faculty of Engineering Sciences
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A thermodynamic assessment of the ternary Fe–Ni–Ti system together with a partial reassessment of the binary sub-systems Ni–Ti and Fe–Ti was made following the CALPHAD method and using the compound energy formalism (CEF). Two and four sublattices were used to model the bcc and fcc phases respectively. This allows describing the order–disorder transformations occurring not only in the ternary Fe–Ni–Ti system, but also in the quaternary Al–Fe–Ni–Ti system. The description of the C14 Laves phase TiFe2 was modified to three sublattices in order to be consistent with other Al–Fe–Ni–Ti sub-systems in which a three sublattice model is needed. Thermodynamic parameters were optimized using the available experimental data. On the basis of this optimization the stable phase diagram is calculated. Moreover stable and metastable equilibria between ordered and disordered phases based on fcc and bcc respectively are calculated.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.calphad.2008.10.003

Chinese Library Classification Number:

Citation Information:

A thermodynamic assessment of the ternary Fe–Ni–Ti system together with a partial reassessment of the binary sub-systems Ni–Ti and Fe–Ti was made following the CALPHAD method and using the compound energy formalism (CEF). Two and four sublattices were used to model the bcc and fcc phases respectively. This allows describing the order–disorder transformations occurring not only in the ternary Fe–Ni–Ti system, but also in the quaternary Al–Fe–Ni–Ti system. The description of the C14 Laves phase TiFe2 was modified to three sublattices in order to be consistent with other Al–Fe–Ni–Ti sub-systems in which a three sublattice model is needed. Thermodynamic parameters were optimized using the available experimental data. On the basis of this optimization the stable phase diagram is calculated. Moreover stable and metastable equilibria between ordered and disordered phases based on fcc and bcc respectively are calculated.

quote

GB/T 7714-2015 [1] Jozefien De Keyzer, Gabriele Cacciamani, Nathalie Dupin, et al. Calphad, 2009(33). DOI:10.1016/j.calphad.2008.10.003.
MLA [1] Jozefien De Keyzer, et al., Calphad, no. 33, 2009, https://doi.org/10.1016/j.calphad.2008.10.003.
APA [1] Jozefien De Keyzer, Gabriele Cacciamani, Nathalie Dupin, & Patrick Wollants. (2009). Calphad(33). https://doi.org/10.1016/j.calphad.2008.10.003
IEEE [1] Jozefien De Keyzer, Gabriele Cacciamani, Nathalie Dupin, and Patrick Wollants, Calphad, no. 33, 2009, doi: 10.1016/j.calphad.2008.10.003.