Predictions of the Al-rich region of the Al–Co–Ni–Y system based upon first-principles and experimental data AITranslate

University Park; University Park; University Park; University Park
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A thermodynamic database has been produced for the Al–Co–Ni–Y quaternary system, with an emphasis on the Al-rich region of the Al–Ni–Y ternary system. The database was created using the CALPHAD method, combining existing binary systems with relevant experimental and first-principles information for selected Al–Ni–Y and Co-containing compounds. The thermodynamic database was used to produce equilibrium and non-equilibrium Scheil simulations to determine the phases present in Al–Co–Ni–Y alloys. The values for the Scheil simulation show good agreement, when compared with experimentally determined phase fractions of intermetallic particles dispersed in an Al matrix for three Al-rich quaternary alloys.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.calphad.2008.09.001

Chinese Library Classification Number:

Citation Information:

A thermodynamic database has been produced for the Al–Co–Ni–Y quaternary system, with an emphasis on the Al-rich region of the Al–Ni–Y ternary system. The database was created using the CALPHAD method, combining existing binary systems with relevant experimental and first-principles information for selected Al–Ni–Y and Co-containing compounds. The thermodynamic database was used to produce equilibrium and non-equilibrium Scheil simulations to determine the phases present in Al–Co–Ni–Y alloys. The values for the Scheil simulation show good agreement, when compared with experimentally determined phase fractions of intermetallic particles dispersed in an Al matrix for three Al-rich quaternary alloys.

quote

GB/T 7714-2015 [1] W.J. Golumbfskie, S.N. Prins, T.J. Eden, et al. Calphad, 2009(33). DOI:10.1016/j.calphad.2008.09.001.
MLA [1] W.J. Golumbfskie, et al., Calphad, no. 33, 2009, https://doi.org/10.1016/j.calphad.2008.09.001.
APA [1] W.J. Golumbfskie, S.N. Prins, T.J. Eden, & Z.K. Liu. (2009). Calphad(33). https://doi.org/10.1016/j.calphad.2008.09.001
IEEE [1] W.J. Golumbfskie, S.N. Prins, T.J. Eden, and Z.K. Liu, Calphad, no. 33, 2009, doi: 10.1016/j.calphad.2008.09.001.