We report membranes with ultrathin <200 nm zwitterionic copolymer selective layers exhibiting ∼1 nm size cutoff and permeances as high as 50 L/m2·hr·bar. The thin layer is formed by the deposition of random zwitterionic copolymers in trifluoroethanol/ionic liquid mixtures onto a porous support. The resultant membranes have the same low molecular weight cutoff of ∼1000 Da and narrow pore size distribution but fluxes up to 10 times higher than membranes prepared without ionic liquid and 20 times higher than commercial membranes of similar pore size, making them promising for wastewater treatment and pharmaceutical purification.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.9b00409
Chinese Library Classification Number:
Citation Information:
We report membranes with ultrathin <200 nm zwitterionic copolymer selective layers exhibiting ∼1 nm size cutoff and permeances as high as 50 L/m2·hr·bar. The thin layer is formed by the deposition of random zwitterionic copolymers in trifluoroethanol/ionic liquid mixtures onto a porous support. The resultant membranes have the same low molecular weight cutoff of ∼1000 Da and narrow pore size distribution but fluxes up to 10 times higher than membranes prepared without ionic liquid and 20 times higher than commercial membranes of similar pore size, making them promising for wastewater treatment and pharmaceutical purification.
quote
| GB/T 7714-2015 | [1] Prity BenganiLutz, Ilin Sadeghi, Samuel J. Lounder, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00409. |
| MLA | [1] Prity BenganiLutz, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00409. |
| APA | [1] Prity BenganiLutz, Ilin Sadeghi, Samuel J. Lounder, Matthew J. Panzer, & Ayse Asatekin. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00409 |