Streamlined Fabrication of Asymmetric Carbon Molecular Sieve Hollow Fiber Membranes AITranslate
Abstract AITranslate
A microporous polymer, polymer of intrinsic microporosity-1, was utilized as the polymeric precursor to simplify the formation of asymmetric carbon molecular sieve hollow fiber membranes. Unlike other methods, asymmetric carbon membranes were formed directly without cross-linking or other pretreatments. In addition, a facile defect removal treatment was developed that can easily be incorporated into a standard fiber solvent exchange procedure. The resulting asymmetric carbon membranes display extraordinary gas selectivities at or exceeding the upper bound for O2/N2, CO2/CH4, He/N2, and C2H4/C2H6. The simplified, two-step method greatly improves the ease of fabrication of defect-free asymmetric carbon hollow fiber membranes for challenging separations.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.9b00567
Chinese Library Classification Number:
Citation Information:
A microporous polymer, polymer of intrinsic microporosity-1, was utilized as the polymeric precursor to simplify the formation of asymmetric carbon molecular sieve hollow fiber membranes. Unlike other methods, asymmetric carbon membranes were formed directly without cross-linking or other pretreatments. In addition, a facile defect removal treatment was developed that can easily be incorporated into a standard fiber solvent exchange procedure. The resulting asymmetric carbon membranes display extraordinary gas selectivities at or exceeding the upper bound for O2/N2, CO2/CH4, He/N2, and C2H4/C2H6. The simplified, two-step method greatly improves the ease of fabrication of defect-free asymmetric carbon hollow fiber membranes for challenging separations.
quote
| GB/T 7714-2015 | [1] Melinda L. Jue, Yao Ma, Ryan P. Lively. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00567. |
| MLA | [1] Melinda L. Jue, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00567. |
| APA | [1] Melinda L. Jue, Yao Ma, & Ryan P. Lively. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00567 |
| IEEE | [1] Melinda L. Jue, Yao Ma, and Ryan P. Lively, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00567. keywords: {polymers of intrinsic microporosity;carbon molecular sieves;hollow fiber membranes;gas separations;organic separations;Show More} |