Vacuum-Deposited Wide-Bandgap Perovskite for All-Perovskite Tandem Solar Cells AITranslate

University of Cambridge; University of Cambridge; University of Cambridge; University of Cambridge; University of Cambridge; University of Cambridge; University of Cambridge; University of Cambridge
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

All-perovskite tandem solar cells beckon as lower cost alternatives to conventional single-junction cells. Solution processing has enabled rapid optimization of perovskite solar technologies, but new deposition routes will enable modularity and scalability, facilitating technology adoption. Here, we utilize 4-source vacuum deposition to deposit FA0.7Cs0.3Pb(IxBr1–x)3 perovskite, where the bandgap is changed through fine control over the halide content. We show how using MeO-2PACz as a hole-transporting material and passivating the perovskite with ethylenediammonium diiodide reduces nonradiative losses, resulting in efficiencies of 17.8% in solar cells based on vacuum-deposited perovskites with a bandgap of 1.76 eV. By similarly passivating a narrow-bandgap FA0.75Cs0.25Pb0.5Sn0.5I3 perovskite and combining it with a subcell of evaporated FA0.7Cs0.3Pb(I0.64Br0.36)3, we report a 2-terminal all-perovskite tandem solar cell with champion open circuit voltage and efficiency of 2.06 V and 24.1%, respectively. This dry deposition method enables high reproducibility, opening avenues for modular, scalable multijunction devices even in complex architectures.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00564

Chinese Library Classification Number:

Citation Information:

All-perovskite tandem solar cells beckon as lower cost alternatives to conventional single-junction cells. Solution processing has enabled rapid optimization of perovskite solar technologies, but new deposition routes will enable modularity and scalability, facilitating technology adoption. Here, we utilize 4-source vacuum deposition to deposit FA0.7Cs0.3Pb(IxBr1–x)3 perovskite, where the bandgap is changed through fine control over the halide content. We show how using MeO-2PACz as a hole-transporting material and passivating the perovskite with ethylenediammonium diiodide reduces nonradiative losses, resulting in efficiencies of 17.8% in solar cells based on vacuum-deposited perovskites with a bandgap of 1.76 eV. By similarly passivating a narrow-bandgap FA0.75Cs0.25Pb0.5Sn0.5I3 perovskite and combining it with a subcell of evaporated FA0.7Cs0.3Pb(I0.64Br0.36)3, we report a 2-terminal all-perovskite tandem solar cell with champion open circuit voltage and efficiency of 2.06 V and 24.1%, respectively. This dry deposition method enables high reproducibility, opening avenues for modular, scalable multijunction devices even in complex architectures.

quote

GB/T 7714-2015 [1] YuHsien Chiang, Kyle Frohna, Hayden Salway, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00564.
MLA [1] YuHsien Chiang, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00564.
APA [1] YuHsien Chiang, Kyle Frohna, Hayden Salway, Anna Abfalterer, Linfeng Pan, Bart Roose, Miguel Anaya, & Samuel D. Stranks. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00564
IEEE [1] YuHsien Chiang, Kyle Frohna, Hayden Salway, Anna Abfalterer, Linfeng Pan, Bart Roose, Miguel Anaya, and Samuel D. Stranks, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00564.