Exploiting Fluoropolymers Immiscibility to Tune Surface Properties and Mass Transfer in Blend Membranes for Membrane Contactor Applications AITranslate

Institute on Membrane Technology (ITM); Institute on Membrane Technology (ITM); Institute on Membrane Technology (ITM); Institute on Membrane Technology (ITM); University of Calabria; University of Calabria (UNICAL); University of Calabria (UNICAL); Institute on Membrane Technology (ITM)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Polyvinylidene fluoride-co-hexafluoropropylene (PVDF-HFP) and polyvinylidene fluoride (PVDF) blend membranes, with interconnected channels decorated with polymer crystallites, were produced by a two-step phase separation technique, using nontoxic solvents and without any chemical additive as pore forming. Results demonstrated that the mass-transport and the interface properties of the membranes can be tailored by a synergic combination of immiscible blend components and an adequate manufacturing procedure, that exploit the slow diffusion of the nonsolvent by vapor induced phase separation. In this way, multilevel hierarchical surfaces, with raspberry- and cauliflower-like substructures, were obtained. The optimal blending ratio between the two components was assessed by chemical physical and mass-transport property characterizations of the prepared membranes. The beneficial effect of blending was evidenced for all the properties investigated (crystallinity, surface roughness, wettability, surface charge, strength, toughness, and flux), indicating a good physical interaction between the two components, despite their thermodynamically stated immiscibility. This physical interaction was also proved by the presence of PVDF crystallites embedded in the PVDF-HFP network of blend membranes, which act as reinforcing agents rather than as independent fillers with respect to the pure copolymer, providing enhanced mechanical properties.

KeyWords AITranslate

PVDF PVDFHFP polymers blending solubility parameters membrane contactor miscibility surface roughness wettability
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.8b00105

Chinese Library Classification Number:

Citation Information:

Polyvinylidene fluoride-co-hexafluoropropylene (PVDF-HFP) and polyvinylidene fluoride (PVDF) blend membranes, with interconnected channels decorated with polymer crystallites, were produced by a two-step phase separation technique, using nontoxic solvents and without any chemical additive as pore forming. Results demonstrated that the mass-transport and the interface properties of the membranes can be tailored by a synergic combination of immiscible blend components and an adequate manufacturing procedure, that exploit the slow diffusion of the nonsolvent by vapor induced phase separation. In this way, multilevel hierarchical surfaces, with raspberry- and cauliflower-like substructures, were obtained. The optimal blending ratio between the two components was assessed by chemical physical and mass-transport property characterizations of the prepared membranes. The beneficial effect of blending was evidenced for all the properties investigated (crystallinity, surface roughness, wettability, surface charge, strength, toughness, and flux), indicating a good physical interaction between the two components, despite their thermodynamically stated immiscibility. This physical interaction was also proved by the presence of PVDF crystallites embedded in the PVDF-HFP network of blend membranes, which act as reinforcing agents rather than as independent fillers with respect to the pure copolymer, providing enhanced mechanical properties.

quote

GB/T 7714-2015 [1] Carmen Meringolo, Teresa Poerio, Enrica Fontananova, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.8b00105.
MLA [1] Carmen Meringolo, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.8b00105.
APA [1] Carmen Meringolo, Teresa Poerio, Enrica Fontananova, Teresa F. Mastropietro, Fiore P. Nicoletta, Giovanni De Filpo, Efrem Curcio, & Gianluca Di Profio. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.8b00105
IEEE [1] Carmen Meringolo, Teresa Poerio, Enrica Fontananova, Teresa F. Mastropietro, Fiore P. Nicoletta, Giovanni De Filpo, Efrem Curcio, and Gianluca Di Profio, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.8b00105. keywords: {PVDF;PVDFHFP;polymers blending;solubility parameters;membrane contactor;miscibility;surface roughness;wettability}