Air Templated Macroporous Epoxy Foams with Silica Particles as Property-Defining Additive AITranslate

University of Vienna; University of Vienna; University of Vienna
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Nonaqueous foams were successfully produced by mechanically beating air into liquid epoxy resin, surfactant, and silica particle mixtures and used as templates to produce macroporous polymers. The air bubbles introduced into the epoxy formulations served as templates for the pores of the cured epoxy foams. The addition of silica particles into the resin mixture resulted in an increased viscosity of the formulation, thus enhancing the stability of the liquid epoxy froths, which could then be thermally cured at 60 °C. Increasing the silica loading in the formulation resulted in an increase of the foam density and decrease of the average pore size of the epoxy foams. The epoxy foams containing silica exhibited a hierarchical pore structure, where large pores were surrounded by smaller pores, and enhanced stiffness as compared to the control epoxy foams with a monomodal pore size distribution.

KeyWords AITranslate

epoxy foam nonaqueous foams frothing hierarchical porous structure templating
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.8b00084

Chinese Library Classification Number:

Citation Information:

Nonaqueous foams were successfully produced by mechanically beating air into liquid epoxy resin, surfactant, and silica particle mixtures and used as templates to produce macroporous polymers. The air bubbles introduced into the epoxy formulations served as templates for the pores of the cured epoxy foams. The addition of silica particles into the resin mixture resulted in an increased viscosity of the formulation, thus enhancing the stability of the liquid epoxy froths, which could then be thermally cured at 60 °C. Increasing the silica loading in the formulation resulted in an increase of the foam density and decrease of the average pore size of the epoxy foams. The epoxy foams containing silica exhibited a hierarchical pore structure, where large pores were surrounded by smaller pores, and enhanced stiffness as compared to the control epoxy foams with a monomodal pore size distribution.

quote

GB/T 7714-2015 [1] Mohammad Jalalian, Qixiang Jiang, Alexander Bismarck. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.8b00084.
MLA [1] Mohammad Jalalian, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.8b00084.
APA [1] Mohammad Jalalian, Qixiang Jiang, & Alexander Bismarck. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.8b00084
IEEE [1] Mohammad Jalalian, Qixiang Jiang, and Alexander Bismarck, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.8b00084. keywords: {epoxy foam;nonaqueous foams;frothing;hierarchical porous structure;templating}