The Dark Side of Lead-Free Metal Halide Nanocrystals: Substituent-Modulated Photocatalytic Activity in Benzyl Bromide Reduction AITranslate
Abstract AITranslate
We illustrate here the high photocatalytic activity of sustainable lead-free metal halide nanocrystals (NCs), namely, Cs3Sb2Br9 NCs, in the reduction of p-substituted benzyl bromides in the absence of a cocatalyst. The electronic properties of the benzyl bromide substituents and the substrate affinity to the NC surface determine the selectivity in C–C homocoupling under visible light irradiation. This photocatalyst can be reused for at least three cycles and preserves its good performance with a turnover number of ca. 105,000.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.3c00771
Chinese Library Classification Number:
Citation Information:
We illustrate here the high photocatalytic activity of sustainable lead-free metal halide nanocrystals (NCs), namely, Cs3Sb2Br9 NCs, in the reduction of p-substituted benzyl bromides in the absence of a cocatalyst. The electronic properties of the benzyl bromide substituents and the substrate affinity to the NC surface determine the selectivity in C–C homocoupling under visible light irradiation. This photocatalyst can be reused for at least three cycles and preserves its good performance with a turnover number of ca. 105,000.
quote
| GB/T 7714-2015 | [1] Ignacio RosaPardo, Dongxu Zhu, Alejandro CortésVillena, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00771. |
| MLA | [1] Ignacio RosaPardo, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00771. |
| APA | [1] Ignacio RosaPardo, Dongxu Zhu, Alejandro CortésVillena, Mirko Prato, Luca De Trizio, Liberato Manna, Raquel E. Galian, & Julia PérezPrieto. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00771 |
| IEEE | [1] Ignacio RosaPardo, Dongxu Zhu, Alejandro CortésVillena, Mirko Prato, Luca De Trizio, Liberato Manna, Raquel E. Galian, and Julia PérezPrieto, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00771. |