Expanding Interlayer Spacing in MoS2 for Realizing an Advanced Supercapacitor AITranslate
Abstract AITranslate
Charge-storage mechanism of free-standing MoS2/r-GO (r-GO = reduced graphene oxide) hybrid nanoflakes on molybdenum (Mo) foil in Na2SO4 solution is elucidated for realizing a high-performance asymmetric supercapacitor (ASC). Thiourea that acts primarily as sulfur source also helps intercalating ammonium ions, which along with r-GO facilitate in situ exfoliation of MoS2, producing hierarchical MoS2 with expanded interlayer spacing. This interlayer expansion in MoS2 facilitates Na+-ions intercalation/deintercalation and ensures enhanced capacitance, rate capability, and cycling stability of the capacitor. Besides exhibiting attractive energy-cum-power traits, the 2 V MoS2/r-GO//Fe2O3/MnO2 ASC shows compelling cycling performance for over 20 000 cycles in an aqueous electrolyte.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.9b00983
Chinese Library Classification Number:
Citation Information:
Charge-storage mechanism of free-standing MoS2/r-GO (r-GO = reduced graphene oxide) hybrid nanoflakes on molybdenum (Mo) foil in Na2SO4 solution is elucidated for realizing a high-performance asymmetric supercapacitor (ASC). Thiourea that acts primarily as sulfur source also helps intercalating ammonium ions, which along with r-GO facilitate in situ exfoliation of MoS2, producing hierarchical MoS2 with expanded interlayer spacing. This interlayer expansion in MoS2 facilitates Na+-ions intercalation/deintercalation and ensures enhanced capacitance, rate capability, and cycling stability of the capacitor. Besides exhibiting attractive energy-cum-power traits, the 2 V MoS2/r-GO//Fe2O3/MnO2 ASC shows compelling cycling performance for over 20 000 cycles in an aqueous electrolyte.
quote
| GB/T 7714-2015 | [1] Debasish Sarkar, Debanjan Das, Shyamashis Das, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00983. |
| MLA | [1] Debasish Sarkar, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00983. |
| APA | [1] Debasish Sarkar, Debanjan Das, Shyamashis Das, Ankit Kumar, Satish Patil, Karuna Kar Nanda, D. D. Sarma, & Ashok Shukla. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00983 |
| IEEE | [1] Debasish Sarkar, Debanjan Das, Shyamashis Das, Ankit Kumar, Satish Patil, Karuna Kar Nanda, D. D. Sarma, and Ashok Shukla, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00983. |