China|Tianmu Lake Institute of Advanced Energy Storage Technologies Co. Ltd.; Institute of Physics; University of Chinese Academy of Sciences; University of Chinese Academy of Sciences; Institute of Physics; Institute of Physics; University of Chinese Academy of Sciences; University of Chinese Academy of Sciences; University of Chinese Academy of Sciences
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Solid polymer electrolytes (SPEs) are considered as promising candidates for solid-state batteries. SPEs with a conventional solution casting technique have serious side reactions during charging because of the residual solvent. Here we report a creative method that can self-remove it via spontaneous reactions. The core idea is to consume the residual solvent and form stable products by choosing proper salt, solvent, and additives. Inspired by the hydrolysis of sodium bis(fluorosulfonyl)imide (NaFSI), during which the proton carrier changes from H2O to HF and HF further reacts with metal oxide to form a stable hydrate, like AlF3·6H2O, NaFSI, H2O, and Al2O3/SiO2 nanoparticles are thus employed to prepare poly(ethylene oxide) (PEO)-based SPEs. Solid-state sodium batteries with PEO/NaFSI-Al2O3-AQ electrolytes exhibit good reversibility with Na3V2(PO4)3 as the active materials, high rate performance, long-term cycling stability (92.8% after 2000 cycle), and high Coulombic efficiency. Furthermore, environmentally friendly and low-cost preparation of PEO-based SPEs is realized with this aqueous technique.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b00857

Chinese Library Classification Number:

Citation Information:

Solid polymer electrolytes (SPEs) are considered as promising candidates for solid-state batteries. SPEs with a conventional solution casting technique have serious side reactions during charging because of the residual solvent. Here we report a creative method that can self-remove it via spontaneous reactions. The core idea is to consume the residual solvent and form stable products by choosing proper salt, solvent, and additives. Inspired by the hydrolysis of sodium bis(fluorosulfonyl)imide (NaFSI), during which the proton carrier changes from H2O to HF and HF further reacts with metal oxide to form a stable hydrate, like AlF3·6H2O, NaFSI, H2O, and Al2O3/SiO2 nanoparticles are thus employed to prepare poly(ethylene oxide) (PEO)-based SPEs. Solid-state sodium batteries with PEO/NaFSI-Al2O3-AQ electrolytes exhibit good reversibility with Na3V2(PO4)3 as the active materials, high rate performance, long-term cycling stability (92.8% after 2000 cycle), and high Coulombic efficiency. Furthermore, environmentally friendly and low-cost preparation of PEO-based SPEs is realized with this aqueous technique.

quote

GB/T 7714-2015 [1] Lilu Liu, Xingguo Qi, Shijun Yin, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00857.
MLA [1] Lilu Liu, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00857.