Homogeneous Interface Conductivity for Lithium Dendrite-Free Anode AITranslate
Abstract AITranslate
Dendrite growth is one of the major problems that hinder the practical application of lithium metal electrodes in rechargeable lithium batteries. Herein, we report that the thin-film Cu3N coating can greatly suppress the lithium dendrite growth on the Cu current collector. Li|Cu and LiFePO4|Cu cells using thin-film Cu3N-modified Cu foil as electrode exhibit improved cyclic stability and low charge–discharge overpotential. A multifaceted investigation demonstrates that Cu3N can convert to Li3N/Cu nanocomposite after initial lithium plating, forming in situ a highly homogeneous conductive network. The peak-force tunneling atomic force microscopy experiments enable the direct measurement of the surface conductivity, confirming the improved distribution uniformity for the Cu3N-modified Cu. These findings suggest that the uniformity of surface electronic conductivity is an important factor for homogeneous lithium plating–stripping, and in situ formation of a nanoconductive network via conversion reaction could be an effective way to smoothen surface conductivity and thus to achieve high uniformity.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b01244
Chinese Library Classification Number:
Citation Information:
Dendrite growth is one of the major problems that hinder the practical application of lithium metal electrodes in rechargeable lithium batteries. Herein, we report that the thin-film Cu3N coating can greatly suppress the lithium dendrite growth on the Cu current collector. Li|Cu and LiFePO4|Cu cells using thin-film Cu3N-modified Cu foil as electrode exhibit improved cyclic stability and low charge–discharge overpotential. A multifaceted investigation demonstrates that Cu3N can convert to Li3N/Cu nanocomposite after initial lithium plating, forming in situ a highly homogeneous conductive network. The peak-force tunneling atomic force microscopy experiments enable the direct measurement of the surface conductivity, confirming the improved distribution uniformity for the Cu3N-modified Cu. These findings suggest that the uniformity of surface electronic conductivity is an important factor for homogeneous lithium plating–stripping, and in situ formation of a nanoconductive network via conversion reaction could be an effective way to smoothen surface conductivity and thus to achieve high uniformity.
quote
| GB/T 7714-2015 | [1] Quan Li, Hongyi Pan, Wenjun Li, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01244. |
| MLA | [1] Quan Li, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01244. |
| APA | [1] Quan Li, Hongyi Pan, Wenjun Li, Yi Wang, Junyang Wang, Jieyun Zheng, Xiqian Yu, Hong Li, & Liquan Chen. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01244 |
| IEEE | [1] Quan Li, Hongyi Pan, Wenjun Li, Yi Wang, Junyang Wang, Jieyun Zheng, Xiqian Yu, Hong Li, and Liquan Chen, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01244. |