Strategy for Boosting Li-Ion Current in Silicon Nanoparticles AITranslate

Stanford University; Yonsei University; Sungkyunkwan University; Sungkyunkwan University; Sungkyunkwan University; Samsung Advanced Institute of Technology; Samsung Advanced Institute of Technology; Nanjing University of Science and Technology; Sungkyunkwan University; Stanford University; Yonsei University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Improvement in the rate capability needs to be addressed for utilization of a Si anode in high-power Li-ion batteries. Regarding the rate capability, its improvement by Si–C nanocomposites seems to be somewhat saturated, thus indicating that the other method should be tried for further enhancement of the rate capability. Here, we introduce Si nanoparticles uniformly coated with nanometer-thick polyacrylonitrile (PAN) with better wettability to liquid electrolytes and minimizing electronic resistance, which might result from a thick PAN coating: the effective contact surface area made by the contact of Si nanoparticles and liquid electrolyte is increased for larger Li-ion current, leading to ultrafast rate capability retaining 62% of the 0.2C rate discharge capacity at 100C. In addition, a strong adhesive property of PAN provides highly mechanically robust Si anodes for multielectrode-stacked flexible lithium-ion batteries, which show no physical damage after 30 000 bending cycles with a bending radius of 25 mm.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01114

Chinese Library Classification Number:

Citation Information:

Improvement in the rate capability needs to be addressed for utilization of a Si anode in high-power Li-ion batteries. Regarding the rate capability, its improvement by Si–C nanocomposites seems to be somewhat saturated, thus indicating that the other method should be tried for further enhancement of the rate capability. Here, we introduce Si nanoparticles uniformly coated with nanometer-thick polyacrylonitrile (PAN) with better wettability to liquid electrolytes and minimizing electronic resistance, which might result from a thick PAN coating: the effective contact surface area made by the contact of Si nanoparticles and liquid electrolyte is increased for larger Li-ion current, leading to ultrafast rate capability retaining 62% of the 0.2C rate discharge capacity at 100C. In addition, a strong adhesive property of PAN provides highly mechanically robust Si anodes for multielectrode-stacked flexible lithium-ion batteries, which show no physical damage after 30 000 bending cycles with a bending radius of 25 mm.

quote

GB/T 7714-2015 [1] MinSang Song, Geewoo Chang, DaeWoong Jung, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01114.
MLA [1] MinSang Song, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01114.
APA [1] MinSang Song, Geewoo Chang, DaeWoong Jung, MoonSeok Kwon, Ping Li, JunHwan Ku, JaeMan Choi, Kan Zhang, GiRa Yi, Yi Cui, & Jong Hyeok Park. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01114
IEEE [1] MinSang Song, Geewoo Chang, DaeWoong Jung, MoonSeok Kwon, Ping Li, JunHwan Ku, JaeMan Choi, Kan Zhang, GiRa Yi, Yi Cui, and Jong Hyeok Park, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01114.