Facile-Effective Hole-Transporting Materials Based on Dibenzo[a,c]carbazole: The Key Role of Linkage Position to Photovoltaic Performance of Perovskite Solar Cells AITranslate
Abstract AITranslate
The film morphology of the hole-transporting layer is proved to be the key element to charge transfer and the interfacial property in perovskite solar cells. In this Letter, a new dibenzo[a,c]carbazole (DBC) core with multiple reaction sites has been formed with a Y-shape, in which the phenanthrene group was integrated as a plane π structure into the common carbazole moiety. Accordingly, three DBC-based hole-transporting materials (HTMs) with varied molecular configurations were synthesized by the introduction of N-(4-methoxyphenyl)-9,9-dimethyl-9H-fluoren-2-amine (F(Me)NPh) as the periphery group at different linkage positions. Once applied to perovskite solar cells as HTMs, DBC-2 with the twisted and asymmetric structure achieved the highest conversion efficiency of 20.02%. Also, the corresponding dopant-free device exhibited a PCE of 16.43% and good device stability under glovebox and ambient conditions.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.9b01539
Chinese Library Classification Number:
Citation Information:
The film morphology of the hole-transporting layer is proved to be the key element to charge transfer and the interfacial property in perovskite solar cells. In this Letter, a new dibenzo[a,c]carbazole (DBC) core with multiple reaction sites has been formed with a Y-shape, in which the phenanthrene group was integrated as a plane π structure into the common carbazole moiety. Accordingly, three DBC-based hole-transporting materials (HTMs) with varied molecular configurations were synthesized by the introduction of N-(4-methoxyphenyl)-9,9-dimethyl-9H-fluoren-2-amine (F(Me)NPh) as the periphery group at different linkage positions. Once applied to perovskite solar cells as HTMs, DBC-2 with the twisted and asymmetric structure achieved the highest conversion efficiency of 20.02%. Also, the corresponding dopant-free device exhibited a PCE of 16.43% and good device stability under glovebox and ambient conditions.
quote
| GB/T 7714-2015 | [1] Fan Liu, Fei Wu, Weidong Ling, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01539. |
| MLA | [1] Fan Liu, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01539. |
| APA | [1] Fan Liu, Fei Wu, Weidong Ling, Zongxiao Tu, Jianqi Zhang, Zhixiang Wei, Linna Zhu, Qianqian Li, & Zhen Li. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01539 |
| IEEE | [1] Fan Liu, Fei Wu, Weidong Ling, Zongxiao Tu, Jianqi Zhang, Zhixiang Wei, Linna Zhu, Qianqian Li, and Zhen Li, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01539. |