BiVO4 Surface Reduction upon Water Exposure AITranslate

Technical University Darmstadt; Catalonia Institute for Energy Research (IREC); Technical University Darmstadt; Technical University Darmstadt
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The (photo)electrochemical water-splitting mechanism has not yet been completely resolved on an atomic level, partly because the interaction between water and the (photo)electrocatalytic surface has not yet been completely elucidated. Because of its ability to oxidize water upon light exposure, BiVO4 was chosen in this work as a prototype photocatalytic material to investigate the effects of water on a pristine metal oxide surface. In particular, polycrystalline surface-cleaned BiVO4 samples were exposed to water in controlled experiments at room temperature and at 77 K, analyzing any electronic and chemical changes at the surface by applying photoelectron spectroscopy. The results show that upon water exposure, hydroxide species form, the Fermi level position rises, the amount of oxygen at the surface decreases, and bismuth and vanadium partially reduces. Accordingly, the interaction of water with bismuth vanadate seemingly follows a reductive water dissociation process.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01667

Chinese Library Classification Number:

Citation Information:

The (photo)electrochemical water-splitting mechanism has not yet been completely resolved on an atomic level, partly because the interaction between water and the (photo)electrocatalytic surface has not yet been completely elucidated. Because of its ability to oxidize water upon light exposure, BiVO4 was chosen in this work as a prototype photocatalytic material to investigate the effects of water on a pristine metal oxide surface. In particular, polycrystalline surface-cleaned BiVO4 samples were exposed to water in controlled experiments at room temperature and at 77 K, analyzing any electronic and chemical changes at the surface by applying photoelectron spectroscopy. The results show that upon water exposure, hydroxide species form, the Fermi level position rises, the amount of oxygen at the surface decreases, and bismuth and vanadium partially reduces. Accordingly, the interaction of water with bismuth vanadate seemingly follows a reductive water dissociation process.

quote

GB/T 7714-2015 [1] Yannick Hermans, Sebastián MurciaLópez, Andreas Klein, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01667.
MLA [1] Yannick Hermans, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01667.
APA [1] Yannick Hermans, Sebastián MurciaLópez, Andreas Klein, & Wolfram Jaegermann. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01667
IEEE [1] Yannick Hermans, Sebastián MurciaLópez, Andreas Klein, and Wolfram Jaegermann, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01667.