Single-Ion Homopolymer Electrolytes with High Transference Number Prepared by Click Chemistry and Photoinduced Metal-Free Atom-Transfer Radical Polymerization AITranslate

Carnegie Mellon University; Carnegie Mellon University; Carnegie Mellon University; Carnegie Mellon University; Carnegie Mellon University; Carnegie Mellon University; Carnegie Mellon University; Carnegie Mellon University; Carnegie Mellon University; Carnegie Mellon University; Carnegie Mellon University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Solvent-free single-ion polymer electrolytes with high conductivity have historically been prepared in the form of block copolymer or polymer blends. In this work, single-ion homopolymer electrolytes consisting of poly(poly(ethylene oxide) methacrylate lithium sulfonyl(trifluoromethylsulfonyl)imide), poly(PEOMA-TFSI–Li+), were prepared for the first time by photoinduced metal-free atom-transfer radical polymerization. The PEO-based macromonomer PEOMA-TFSI–Li+ was synthesized via click chemistry, copper-catalyzed alkyne–azide cycloaddition. Because of the conductive, amorphous PEO phase in which the lithium ions are located, these polymers showed improved ionic conductivity (10–5–10–4 S/cm at 90 °C) and high transference number (0.97–0.99). A continued lithium plating–stripping experiment was performed at current density ≥0.1 mA/cm2 over 300 cycles at 90 °C. The potential dendrite-suppressing capability of the polymer with such high transference number was also estimated by employing a kinetic model using the measured transport and transference properties to study the current density at the dendrite tip. The analysis indicates that the synthesized polymers could have a high propensity to suppress dendrite growth.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.7b00999

Chinese Library Classification Number:

Citation Information:

Solvent-free single-ion polymer electrolytes with high conductivity have historically been prepared in the form of block copolymer or polymer blends. In this work, single-ion homopolymer electrolytes consisting of poly(poly(ethylene oxide) methacrylate lithium sulfonyl(trifluoromethylsulfonyl)imide), poly(PEOMA-TFSI–Li+), were prepared for the first time by photoinduced metal-free atom-transfer radical polymerization. The PEO-based macromonomer PEOMA-TFSI–Li+ was synthesized via click chemistry, copper-catalyzed alkyne–azide cycloaddition. Because of the conductive, amorphous PEO phase in which the lithium ions are located, these polymers showed improved ionic conductivity (10–5–10–4 S/cm at 90 °C) and high transference number (0.97–0.99). A continued lithium plating–stripping experiment was performed at current density ≥0.1 mA/cm2 over 300 cycles at 90 °C. The potential dendrite-suppressing capability of the polymer with such high transference number was also estimated by employing a kinetic model using the measured transport and transference properties to study the current density at the dendrite tip. The analysis indicates that the synthesized polymers could have a high propensity to suppress dendrite growth.

quote

GB/T 7714-2015 [1] Sipei Li, Alexander I. Mohamed, Vikram Pande, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.7b00999.
MLA [1] Sipei Li, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.7b00999.
APA [1] Sipei Li, Alexander I. Mohamed, Vikram Pande, Han Wang, Julia Cuthbert, Xiangcheng Pan, Hongkun He, Zongyu Wang, Venkatasubramanian Viswanathan, Jay F. Whitacre, & Krzysztof Matyjaszewski. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.7b00999
IEEE [1] Sipei Li, Alexander I. Mohamed, Vikram Pande, Han Wang, Julia Cuthbert, Xiangcheng Pan, Hongkun He, Zongyu Wang, Venkatasubramanian Viswanathan, Jay F. Whitacre, and Krzysztof Matyjaszewski, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.7b00999.