daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Demolded hollow high aspect-ratio parylene-C micropillars for real-time mechanosensing applications AITranslate

Brno University of Technology; Brno University of Technology; Brno University of Technology; Brno University of Technology; Brno University of Technology; Brno University of Technology
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Cells generate mechanical forces to maintain normal cellular function or play a role in developing pathological processes. The mechanical force called the traction force can be estimated from the pillar deflection using a polymeric micropillar array. Here, we develop a transparent membrane of hollow cone-shape high aspect ratio (AR) parylene-C micropillars by the molding method. The membrane of the pillar array is exposed after the etching of the silicon mold and the residual silicon serves as the cultivation chamber. The AR and spring constant (k) of micropillars are estimated to AR ≈ 10 and k ≈ 0.349 N·m−1. The spring constant of developing micropillars is 3.5-times decreased compared to cylindrical, non-hollow pillars. This slightly tune the elastic properties of micropillars. The array is further shown as the mechanosensor detecting the change of cellular tension during hyperosmotic stress. The traction force of cancerous PC-3 cells is estimated from pillar deflections by image analysis. Additionally, the cell volume and surface area are measured using a digital holographic microscope (DHM). The results show that the molding technique can be used to develop high AR parylene-C micropillars and that this array can serve as the mechanosensor of cellular processes. Graphical abstract Download : Download high-res image (176KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2023.101736

Chinese Library Classification Number:

Citation Information:

Cells generate mechanical forces to maintain normal cellular function or play a role in developing pathological processes. The mechanical force called the traction force can be estimated from the pillar deflection using a polymeric micropillar array. Here, we develop a transparent membrane of hollow cone-shape high aspect ratio (AR) parylene-C micropillars by the molding method. The membrane of the pillar array is exposed after the etching of the silicon mold and the residual silicon serves as the cultivation chamber. The AR and spring constant (k) of micropillars are estimated to AR ≈ 10 and k ≈ 0.349 N·m−1. The spring constant of developing micropillars is 3.5-times decreased compared to cylindrical, non-hollow pillars. This slightly tune the elastic properties of micropillars. The array is further shown as the mechanosensor detecting the change of cellular tension during hyperosmotic stress. The traction force of cancerous PC-3 cells is estimated from pillar deflections by image analysis. Additionally, the cell volume and surface area are measured using a digital holographic microscope (DHM). The results show that the molding technique can be used to develop high AR parylene-C micropillars and that this array can serve as the mechanosensor of cellular processes. Graphical abstract Download : Download high-res image (176KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Larisa Chmelikova, Peter Fecko, Jiri Chmelik, et al. Applied Materials Today, 2023(31). DOI:10.1016/j.apmt.2023.101736.
MLA [1] Larisa Chmelikova, et al., Applied Materials Today, no. 31, 2023, https://doi.org/10.1016/j.apmt.2023.101736.
APA [1] Larisa Chmelikova, Peter Fecko, Jiri Chmelik, Josef Skacel, Alexandr Otahal, & Zdenka Fohlerova. (2023). Applied Materials Today(31). https://doi.org/10.1016/j.apmt.2023.101736
IEEE [1] Larisa Chmelikova, Peter Fecko, Jiri Chmelik, Josef Skacel, Alexandr Otahal, and Zdenka Fohlerova, Applied Materials Today, no. 31, 2023, doi: 10.1016/j.apmt.2023.101736.