In situ Stress Monitoring Reveals Tension and Wrinkling Evolutions during Halide Perovskite Film Formation AITranslate
Abstract AITranslate
Metal halide perovskites (MHPs) are promising candidates for next-generation thin film photovoltaics and high-performance tandems. Solution-processed MHP films are susceptible to residual stress that can induce undesirable surface wrinkles. However, the origins and evolution of stress during solution processing remain elusive. In this work, we utilize multimodal in situ characterizations, including substrate curvature, reflectance, absorbance, and photoluminescence, to monitor stress and morphology evolution during MHP film formation. A film formation model emerges, consisting of a perovskite top crust on a semirigid sol with the ability to transfer mechanical forces. The phase transformation induces tension in the MHP crust, while shrinkage of the sol causes additional compression and surface wrinkles. Wrinkle-free films are formed through dynamically balancing forces between the crust and the sol. This study provides a powerful toolkit for the fast-growing area of stress engineering in MHP photovoltaics to achieve dynamic control of film stress and surface morphology.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.3c02079
Chinese Library Classification Number:
Citation Information:
Metal halide perovskites (MHPs) are promising candidates for next-generation thin film photovoltaics and high-performance tandems. Solution-processed MHP films are susceptible to residual stress that can induce undesirable surface wrinkles. However, the origins and evolution of stress during solution processing remain elusive. In this work, we utilize multimodal in situ characterizations, including substrate curvature, reflectance, absorbance, and photoluminescence, to monitor stress and morphology evolution during MHP film formation. A film formation model emerges, consisting of a perovskite top crust on a semirigid sol with the ability to transfer mechanical forces. The phase transformation induces tension in the MHP crust, while shrinkage of the sol causes additional compression and surface wrinkles. Wrinkle-free films are formed through dynamically balancing forces between the crust and the sol. This study provides a powerful toolkit for the fast-growing area of stress engineering in MHP photovoltaics to achieve dynamic control of film stress and surface morphology.
quote
| GB/T 7714-2015 | [1] Boyu Guo, Mihirsinh Chauhan, Nathaniel R. Woodward, et al. ACS Energy Letters, 2024(9). DOI:10.1021/acsenergylett.3c02079. |
| MLA | [1] Boyu Guo, et al., ACS Energy Letters, no. 9, 2024, https://doi.org/10.1021/acsenergylett.3c02079. |
| APA | [1] Boyu Guo, Mihirsinh Chauhan, Nathaniel R. Woodward, Gabriel R. McAndrews, Gaurab J. Thapa, Benjamin M. Lefler, Ruipeng Li, Tonghui Wang, Kasra Darabi, Michael D. McGehee, & Aram Amassian. (2024). ACS Energy Letters(9). https://doi.org/10.1021/acsenergylett.3c02079 |
| IEEE | [1] Boyu Guo, Mihirsinh Chauhan, Nathaniel R. Woodward, Gabriel R. McAndrews, Gaurab J. Thapa, Benjamin M. Lefler, Ruipeng Li, Tonghui Wang, Kasra Darabi, Michael D. McGehee, and Aram Amassian, ACS Energy Letters, no. 9, 2024, doi: 10.1021/acsenergylett.3c02079. |