Flexible Large-Scale Self-Driven Perovskite X-ray Detector by Precise Heterogeneous Integration AITranslate

Shaanxi Normal University; Shaanxi Normal University; Shaanxi Normal University; Shaanxi Normal University; Shaanxi Normal University; Dalian Institute of Chemical Physics; Shaanxi Normal University; Shaanxi Normal University; University of Science and Technology of China; Dalian Institute of Chemical Physics; Shaanxi Normal University; University of Science and Technology of China; Dalian Institute of Chemical Physics; Shaanxi Normal University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Self-driven X-ray detectors, which eliminate the need for an external power supply and offer portability, are gaining significant attention for medical and industrial applications. However, their use is limited in emerging wearable electronics for imaging non-flat or complex objects. Here, we address this issue by developing a heterogeneous integration strategy on a scalable production scale to create flexible, large-scale, and thick perovskite membranes with high-performance, self-driven X-ray detection and imaging capabilities. The precise heterogeneous integration between 3D perovskites and various 2D perovskites can achieve a complex balance among spontaneous charge separation/transport, X-ray attenuation, and mechanical durability. Thus, we provide the first demonstration of a flexible perovskite heterojunction for X-ray detectors with a record self-driven sensitivity of 292 μC Gyair–1 cm–2. Furthermore, we mark the first demonstration of the imaging capability of perovskite self-driven X-ray detectors. This work may provide a foundation for developing a host of sustainable and flexible perovskite optoelectronic devices.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c02152

Chinese Library Classification Number:

Citation Information:

Self-driven X-ray detectors, which eliminate the need for an external power supply and offer portability, are gaining significant attention for medical and industrial applications. However, their use is limited in emerging wearable electronics for imaging non-flat or complex objects. Here, we address this issue by developing a heterogeneous integration strategy on a scalable production scale to create flexible, large-scale, and thick perovskite membranes with high-performance, self-driven X-ray detection and imaging capabilities. The precise heterogeneous integration between 3D perovskites and various 2D perovskites can achieve a complex balance among spontaneous charge separation/transport, X-ray attenuation, and mechanical durability. Thus, we provide the first demonstration of a flexible perovskite heterojunction for X-ray detectors with a record self-driven sensitivity of 292 μC Gyair–1 cm–2. Furthermore, we mark the first demonstration of the imaging capability of perovskite self-driven X-ray detectors. This work may provide a foundation for developing a host of sustainable and flexible perovskite optoelectronic devices.

quote

GB/T 7714-2015 [1] Haojin Li, Xinmei Liu, Tinghuan Yang, et al. ACS Energy Letters, 2024(9). DOI:10.1021/acsenergylett.3c02152.
MLA [1] Haojin Li, et al., ACS Energy Letters, no. 9, 2024, https://doi.org/10.1021/acsenergylett.3c02152.
APA [1] Haojin Li, Xinmei Liu, Tinghuan Yang, Chuang Ma, Yachao Du, Peng Xu, Lu Zhang, Xin Song, Qingyue Cui, Shengli Zhao, Zhou Yang, Shengzhong Frank Liu, Shengye Jin, & Kui Zhao. (2024). ACS Energy Letters(9). https://doi.org/10.1021/acsenergylett.3c02152
IEEE [1] Haojin Li, Xinmei Liu, Tinghuan Yang, Chuang Ma, Yachao Du, Peng Xu, Lu Zhang, Xin Song, Qingyue Cui, Shengli Zhao, Zhou Yang, Shengzhong Frank Liu, Shengye Jin, and Kui Zhao, ACS Energy Letters, no. 9, 2024, doi: 10.1021/acsenergylett.3c02152.