A method of drug delivery to tumors based on rapidly biodegradable drug-loaded containers AITranslate

Saratov State University;Lobachevsky State University of Nizhny Novgorod; Saratov State University; Sechenov University;Lobachevsky State University of Nizhny Novgorod;Lobachevsky State University of Nizhny Novgorod;Institute of Organometallic Chemistry of RAS;Institute of Organometallic Chemistry of RAS; Uppsala University; Uppsala University;Skolkovo Institute of Science and Technology; Queen Mary University of London; Macquarie University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

To mitigate side effects in systemic administration, anticancer drugs are encapuslated in nanocontainers. The nanocontainers are impermeable through normal vessel walls but can permeate and retain in the tumor, albeit their diffusive transport in the tumor interstitium towards pharmacological targets is drastically hindered by the tumor microenvironment resulting in a compromised therapeutic efficacy. We introduce a new drug delivery concept, which relies on drug container passive accumulation in the tumor vasculature followed by an hours-scale release of small-molecule payload that cross the capillary walls to the tumor interstitium and permeates the tumor parenchyma. To demonstrate this approach, a colloidal solution of geology-inspired sub-micron vaterite particles (VPs) loaded with photosensitiser drug porphyrazine was used to deliver and visualise porphyrazine biodistribution in the tumors in vivo. The tumor uptake of polyethylene-glycol-coated gold nanorods and porphyrazine was enhanced c.a 4-fold and 1.8-fold, respectively, when formulated in VP containers. The tumor uptake of ∼30%ID/g much higher than the field average was achieved and enabled successful photodynamic therapy. Graphical abstract Download : Download high-res image (259KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2021.101199

Chinese Library Classification Number:

Citation Information:

To mitigate side effects in systemic administration, anticancer drugs are encapuslated in nanocontainers. The nanocontainers are impermeable through normal vessel walls but can permeate and retain in the tumor, albeit their diffusive transport in the tumor interstitium towards pharmacological targets is drastically hindered by the tumor microenvironment resulting in a compromised therapeutic efficacy. We introduce a new drug delivery concept, which relies on drug container passive accumulation in the tumor vasculature followed by an hours-scale release of small-molecule payload that cross the capillary walls to the tumor interstitium and permeates the tumor parenchyma. To demonstrate this approach, a colloidal solution of geology-inspired sub-micron vaterite particles (VPs) loaded with photosensitiser drug porphyrazine was used to deliver and visualise porphyrazine biodistribution in the tumors in vivo. The tumor uptake of polyethylene-glycol-coated gold nanorods and porphyrazine was enhanced c.a 4-fold and 1.8-fold, respectively, when formulated in VP containers. The tumor uptake of ∼30%ID/g much higher than the field average was achieved and enabled successful photodynamic therapy. Graphical abstract Download : Download high-res image (259KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Bogdan V. Parakhonskiy, Natalia Yu Shilyagina, Оlga I. Gusliakova, et al. Applied Materials Today, 2021(25). DOI:10.1016/j.apmt.2021.101199.
MLA [1] Bogdan V. Parakhonskiy, et al., Applied Materials Today, no. 25, 2021, https://doi.org/10.1016/j.apmt.2021.101199.
APA [1] Bogdan V. Parakhonskiy, Natalia Yu Shilyagina, Оlga I. Gusliakova, Artur B. Volovetskiy, Alexey B. Kostyuk, Irina V. Balalaeva, Larisa G. Klapshina, Svetlana A. Lermontova, Vladimir Tolmachev, Anna Orlova, Dmitry A. Gorin, Gleb B. Sukhorukov, & Andrei V. Zvyagin. (2021). Applied Materials Today(25). https://doi.org/10.1016/j.apmt.2021.101199
IEEE [1] Bogdan V. Parakhonskiy, Natalia Yu Shilyagina, Оlga I. Gusliakova, Artur B. Volovetskiy, Alexey B. Kostyuk, Irina V. Balalaeva, Larisa G. Klapshina, Svetlana A. Lermontova, Vladimir Tolmachev, Anna Orlova, Dmitry A. Gorin, Gleb B. Sukhorukov, and Andrei V. Zvyagin, Applied Materials Today, no. 25, 2021, doi: 10.1016/j.apmt.2021.101199.