Anti-Swelling Zwitterionic Hydrogels as Multi-Modal Underwater Sensors and All-in-One Supercapacitors AITranslate

Zhejiang University of Technology; The University of Akron; Zhejiang University of Technology; Zhejiang University of Technology; Zhejiang University of Technology; Zhejiang University of Technology; Zhejiang University of Technology; Zhejiang University of Technology; Zhejiang University of Technology; Zhejiang University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Although hydrogel-based electronic devices have received a lot of interest for good flexibility, biocompatibility, and multifunctionality over the past decades, underwater instability (especially in saline solutions) still limits their practical applications to a wide range. Herein, a class of tough, conductive, and anti-swelling double-network hydrogel is developed by combining the zwitterionic poly(acrylamide-co-(3-(1-(4-vinylbenzyl)-1H-benzo[d]imidazole-3-ium-3-yl) propane-1-sulfonate)) chemical network and water-resistant polyvinyl alcohol physical network with conducting polypyrrole. The resultant gel exhibits considerable mechanical strength (0.65 MPa), stable swelling dynamics in water and seawater, as well as excellent ionic conductivity (3.96 S/m). Furthermore, the assembled gel-based sensor shows distinct strain/temperature bi-modal detection. Moreover, by controlling the dimension of conductive networks, an all-in-one supercapacitor can be obtained, with ultra-high capacitance (299.79 mF/cm2) and power density (2.49 mW/cm2). We believe that this strategy will inspire researchers to develop more reliable underwater, self-powered multi-modal sensing devices in the future.

KeyWords AITranslate

hydrogel polyzwitterion antiswelling underwater sensor supercapacitor
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01202

Chinese Library Classification Number:

Citation Information:

Although hydrogel-based electronic devices have received a lot of interest for good flexibility, biocompatibility, and multifunctionality over the past decades, underwater instability (especially in saline solutions) still limits their practical applications to a wide range. Herein, a class of tough, conductive, and anti-swelling double-network hydrogel is developed by combining the zwitterionic poly(acrylamide-co-(3-(1-(4-vinylbenzyl)-1H-benzo[d]imidazole-3-ium-3-yl) propane-1-sulfonate)) chemical network and water-resistant polyvinyl alcohol physical network with conducting polypyrrole. The resultant gel exhibits considerable mechanical strength (0.65 MPa), stable swelling dynamics in water and seawater, as well as excellent ionic conductivity (3.96 S/m). Furthermore, the assembled gel-based sensor shows distinct strain/temperature bi-modal detection. Moreover, by controlling the dimension of conductive networks, an all-in-one supercapacitor can be obtained, with ultra-high capacitance (299.79 mF/cm2) and power density (2.49 mW/cm2). We believe that this strategy will inspire researchers to develop more reliable underwater, self-powered multi-modal sensing devices in the future.

quote

GB/T 7714-2015 [1] Shuaibing Wang, Dong Zhang, Xiaomin He, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01202.
MLA [1] Shuaibing Wang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01202.
APA [1] Shuaibing Wang, Dong Zhang, Xiaomin He, Jiahui Zhou, Yimin Zhou, Xiaoyu Wang, Zhu Wang, Shanqiu Liu, Si Yu Zheng, & Jintao Yang. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01202
IEEE [1] Shuaibing Wang, Dong Zhang, Xiaomin He, Jiahui Zhou, Yimin Zhou, Xiaoyu Wang, Zhu Wang, Shanqiu Liu, Si Yu Zheng, and Jintao Yang, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01202. keywords: {hydrogel;polyzwitterion;antiswelling;underwater sensor;supercapacitor}