Guanylation Significantly Enhances the Antifungal Activity of Poly(α-lysine) AITranslate
Abstract AITranslate
AMP-mimicking polymers have the potential to serve as an alternative to small-molecule antifungal drugs. Herein, we synthesized four different molecular weight poly(α-lysine) (α-PLn, n = 1–4) and further modified α-PLn to afford guanylated α-PLn (α-PLn-Gx, where x denotes the percentage of guanylation) with enhanced antifungal activities. α-PLn exhibited good antibacterial activities against Escherichia coli (E. coli) and Staphylococcus aureus (S. aureus), with minimal inhibitory concentration (MIC) values of 24–96 μg/mL, but it did not show antifungal activities against Candida albicans, Candida parapsilosis, Candida krusei, and Candida glabrata, except for Candida tropicalis (MIC < 3 μg/mL). After guanylation, the antifungal activities of α-PLn-Gx against C. albicans, C. krusei, and C. parapsilosis were significantly improved when x ≥ 80 and the MIC values of α-PL3-G100 were reduced by >32-fold, 64-fold, and >16-fold, respectively, compared to that of the corresponding α-PL3. The mechanistic studies demonstrated that α-PL3-G100 disrupted the integrity of cell membranes of C. albicans.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c01205
Chinese Library Classification Number:
Citation Information:
AMP-mimicking polymers have the potential to serve as an alternative to small-molecule antifungal drugs. Herein, we synthesized four different molecular weight poly(α-lysine) (α-PLn, n = 1–4) and further modified α-PLn to afford guanylated α-PLn (α-PLn-Gx, where x denotes the percentage of guanylation) with enhanced antifungal activities. α-PLn exhibited good antibacterial activities against Escherichia coli (E. coli) and Staphylococcus aureus (S. aureus), with minimal inhibitory concentration (MIC) values of 24–96 μg/mL, but it did not show antifungal activities against Candida albicans, Candida parapsilosis, Candida krusei, and Candida glabrata, except for Candida tropicalis (MIC < 3 μg/mL). After guanylation, the antifungal activities of α-PLn-Gx against C. albicans, C. krusei, and C. parapsilosis were significantly improved when x ≥ 80 and the MIC values of α-PL3-G100 were reduced by >32-fold, 64-fold, and >16-fold, respectively, compared to that of the corresponding α-PL3. The mechanistic studies demonstrated that α-PL3-G100 disrupted the integrity of cell membranes of C. albicans.
quote
| GB/T 7714-2015 | [1] Hui Liu, Miaomiao Han, Xiao Liu, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01205. |
| MLA | [1] Hui Liu, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01205. |
| APA | [1] Hui Liu, Miaomiao Han, Xiao Liu, & Shengxiang Ji. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01205 |