daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Influence of ground quartz sand finesses on the formation of poorly ordered calcium silicate hydrate prepared by dynamically hydrothermal synthesis AITranslate

Tsinghua University; Chongqing University; Chongqing University; Chongqing University; Chongqing University; Chongqing University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This study aimed to prepare poorly ordered calcium silicate hydrate (C-S-H) via the hydrothermal synthesis method, using ground quartz sand powder and lime as starting materials. The fineness of quartz sand powder under different grinding time and varied grinding aids content was investigated. It further affected the formation of calcium silicate hydrate. Results showed that the main synthesized product was crystalline dicalcium silicate hydrate (C2SH) with a small amount of C-S-H when quartz sand was ground to 29.95 µm for D50, attributed to the coarse particle size with a low silica reaction rate. Increasing the grinding time and grinding aid content of quartz sand improved the silica reaction rate and accelerated the formation of calcium silicate hydrate. Adding 1‰ grinding aid content would greatly improve the grinding efficiency, and the particle size of quartz sand powder was greatly reduced to the smallest value recorded in this study (D50 was 21.08 µm), which was beneficial to the transformation of C-S-H from C2SH. Meanwhile, C-S-H underwent a change from having a flocculated morphology to a needle-like, short-rod-like and fibrous morphology.

KeyWords AITranslate

Quartz sand Particle size Grinding aid Hydrothermal synthesis Poorly ordered calcium silicate hydrate
No data

Basic Information:

DOI:https://doi.org/10.1016/j.cscm.2023.e02746

Chinese Library Classification Number:

Citation Information:

This study aimed to prepare poorly ordered calcium silicate hydrate (C-S-H) via the hydrothermal synthesis method, using ground quartz sand powder and lime as starting materials. The fineness of quartz sand powder under different grinding time and varied grinding aids content was investigated. It further affected the formation of calcium silicate hydrate. Results showed that the main synthesized product was crystalline dicalcium silicate hydrate (C2SH) with a small amount of C-S-H when quartz sand was ground to 29.95 µm for D50, attributed to the coarse particle size with a low silica reaction rate. Increasing the grinding time and grinding aid content of quartz sand improved the silica reaction rate and accelerated the formation of calcium silicate hydrate. Adding 1‰ grinding aid content would greatly improve the grinding efficiency, and the particle size of quartz sand powder was greatly reduced to the smallest value recorded in this study (D50 was 21.08 µm), which was beneficial to the transformation of C-S-H from C2SH. Meanwhile, C-S-H underwent a change from having a flocculated morphology to a needle-like, short-rod-like and fibrous morphology.

quote

GB/T 7714-2015 [1] Guangxiang Ji, Xiaoqin Peng, Shuping Wang, et al. Case Studies in Construction Materials, 2024(20). DOI:10.1016/j.cscm.2023.e02746.
MLA [1] Guangxiang Ji, et al., Case Studies in Construction Materials, no. 20, 2024, https://doi.org/10.1016/j.cscm.2023.e02746.
APA [1] Guangxiang Ji, Xiaoqin Peng, Shuping Wang, Jingjing Li, Keke Sun, & Huihai Chi. (2024). Case Studies in Construction Materials(20). https://doi.org/10.1016/j.cscm.2023.e02746
IEEE [1] Guangxiang Ji, Xiaoqin Peng, Shuping Wang, Jingjing Li, Keke Sun, and Huihai Chi, Case Studies in Construction Materials, no. 20, 2024, doi: 10.1016/j.cscm.2023.e02746. keywords: {Quartz sand;Particle size;Grinding aid;Hydrothermal synthesis;Poorly ordered calcium silicate hydrate}