daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

High-Performance Epoxy Vitrimers with the Joint Action of Dual Dynamic Covalent Bonds AITranslate

Beijing Institute of Technology; Beijing Institute of Technology; Beijing Institute of Technology; Beijing Institute of Technology; Beijing Institute of Technology; Beijing Institute of Technology; Beijing Institute of Technology; Tsinghua University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Epoxy vitrimers have attracted increasing research attention owing to their stable physical properties, reprocessability, recyclability, and degradability. Among them, rapid self-healing can be achieved in dual dynamic covalent epoxy vitrimers. However, research on the performance and high-strength surface welding of dual dynamic covalent epoxy vitrimers with flexibility is still insufficient. Herein, we report a dual dynamic covalent epoxy vitrimer cocross-linked by dimer acid (DAA) and 3,3′-dithiodipropionic acid (DTDA), named E51-DAAx-DTDAy. The results suggest that the stress relaxation and self-healing speed of vitrimers is improved and the mechanical properties can be restored by 81.2% after 24 h of healing. Additionally, significant recyclability is found in E51-DAAx-DTDAy, with a maximum recovery rate of 119.4% in tensile strength and 124.8% in elongation at break after three times of recycling. Furthermore, Tv of E51-DAAx-DTDAy was above 140 °C; meanwhile, E51-DAAx-DTDAy had better insulation properties, making them more suitable for use as thermosetting materials at moderate temperatures in electronic equipment. E51-DAAx-DTDAy can be recycled by chemical reagents, and green cycling can be achieved. These are attributed to the contributions of disulfide bonds and hydroxyl ester bonds in the network topology.

KeyWords AITranslate

epoxy resin dual dynamic crosslinked network vitrimer selfhealing surface welding
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01738

Chinese Library Classification Number:

Citation Information:

Epoxy vitrimers have attracted increasing research attention owing to their stable physical properties, reprocessability, recyclability, and degradability. Among them, rapid self-healing can be achieved in dual dynamic covalent epoxy vitrimers. However, research on the performance and high-strength surface welding of dual dynamic covalent epoxy vitrimers with flexibility is still insufficient. Herein, we report a dual dynamic covalent epoxy vitrimer cocross-linked by dimer acid (DAA) and 3,3′-dithiodipropionic acid (DTDA), named E51-DAAx-DTDAy. The results suggest that the stress relaxation and self-healing speed of vitrimers is improved and the mechanical properties can be restored by 81.2% after 24 h of healing. Additionally, significant recyclability is found in E51-DAAx-DTDAy, with a maximum recovery rate of 119.4% in tensile strength and 124.8% in elongation at break after three times of recycling. Furthermore, Tv of E51-DAAx-DTDAy was above 140 °C; meanwhile, E51-DAAx-DTDAy had better insulation properties, making them more suitable for use as thermosetting materials at moderate temperatures in electronic equipment. E51-DAAx-DTDAy can be recycled by chemical reagents, and green cycling can be achieved. These are attributed to the contributions of disulfide bonds and hydroxyl ester bonds in the network topology.

quote

GB/T 7714-2015 [1] Xiaoyu Huang, Yichun Wang, Chen Ding, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c01738.
MLA [1] Xiaoyu Huang, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c01738.
APA [1] Xiaoyu Huang, Yichun Wang, Chen Ding, Songmao Zhang, Xiuhui Duan, Hongzeng Ji, Jingyang Cai, & Zixi Wang. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c01738
IEEE [1] Xiaoyu Huang, Yichun Wang, Chen Ding, Songmao Zhang, Xiuhui Duan, Hongzeng Ji, Jingyang Cai, and Zixi Wang, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c01738. keywords: {epoxy resin;dual dynamic crosslinked network;vitrimer;selfhealing;surface welding}