Surfactant-Free Peroxidase-Mediated Enzymatic Polymerization of a Biorenewable Butyrolactone Monomer via a Green Approach: Synthesis of Sustainable Biobased Latexes AITranslate
Abstract AITranslate
A green surfactant-free one-pot horseradish peroxidase-mediated enzymatic polymerization is successfully applied to produce a sustainable and thermally stable biobased high average molar mass poly(α-methylene-γ-butyrolactone) (PMBL) at ambient conditions in water for the first time. The initiation step required only very low concentrations of hydrogen peroxide and 2,4-pentanedione water-soluble initiator to generate the keto-enoxy radicals responsible for forming the primary latex particles. The polymer nanoparticles can be seen as monodisperse, and the biobased latexes are colloidally stable and likely stabilized by the adsorption of 2,4-pentanedione moieties on the particle surfaces. Polymerizations in air produced a 98% yield of PMBL after only 3 h, highlighting the relevance of molecular oxygen. An array of characterization techniques such as dynamic light scattering (DLS), Fourier transform infrared (FTIR), 1H, 13C, and HSQC two-dimensional (2D) nuclear magnetic resonance (NMR), thermogravimetric analysis (TGA), differential scanning calorimetry (DSC), and size-exclusion chromatography (SEC) are used to confirm the properties of the synthesized latexes. The PMBL exhibited high thermal stability, with only a 5% weight loss at 340 °C and a glass-transition temperature of 200 °C, which is double that of polymethyl methacrylate (PMMA). This research provides an interesting pathway for the synthesis of sustainable biobased latexes via enzymes in a green environment using just water at ambient conditions and the potential use of the polymer in high-temperature applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01740
Chinese Library Classification Number:
Citation Information:
A green surfactant-free one-pot horseradish peroxidase-mediated enzymatic polymerization is successfully applied to produce a sustainable and thermally stable biobased high average molar mass poly(α-methylene-γ-butyrolactone) (PMBL) at ambient conditions in water for the first time. The initiation step required only very low concentrations of hydrogen peroxide and 2,4-pentanedione water-soluble initiator to generate the keto-enoxy radicals responsible for forming the primary latex particles. The polymer nanoparticles can be seen as monodisperse, and the biobased latexes are colloidally stable and likely stabilized by the adsorption of 2,4-pentanedione moieties on the particle surfaces. Polymerizations in air produced a 98% yield of PMBL after only 3 h, highlighting the relevance of molecular oxygen. An array of characterization techniques such as dynamic light scattering (DLS), Fourier transform infrared (FTIR), 1H, 13C, and HSQC two-dimensional (2D) nuclear magnetic resonance (NMR), thermogravimetric analysis (TGA), differential scanning calorimetry (DSC), and size-exclusion chromatography (SEC) are used to confirm the properties of the synthesized latexes. The PMBL exhibited high thermal stability, with only a 5% weight loss at 340 °C and a glass-transition temperature of 200 °C, which is double that of polymethyl methacrylate (PMMA). This research provides an interesting pathway for the synthesis of sustainable biobased latexes via enzymes in a green environment using just water at ambient conditions and the potential use of the polymer in high-temperature applications.
quote
| GB/T 7714-2015 | [1] Ahmed Elshewy, Mustapha El Hariri El Nokab, Julien Es Sayed, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c01740. |
| MLA | [1] Ahmed Elshewy, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c01740. |
| APA | [1] Ahmed Elshewy, Mustapha El Hariri El Nokab, Julien Es Sayed, Yasser A. Alassmy, Marwan M. Abduljawad, Dagmar R. D’hooge, Paul H. M. Van Steenberge, Mohamed H. Habib, & Khaled O. Sebakhy. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c01740 |
| IEEE | [1] Ahmed Elshewy, Mustapha El Hariri El Nokab, Julien Es Sayed, Yasser A. Alassmy, Marwan M. Abduljawad, Dagmar R. D’hooge, Paul H. M. Van Steenberge, Mohamed H. Habib, and Khaled O. Sebakhy, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c01740. keywords: {green;sustainability;enzymatic polymerization;butyrolactones;biobased latexes} |