daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Low-Dimensional Organometal Halide Perovskites AITranslate

FAMU-FSU College of Engineering; FAMU-FSU College of Engineering; Florida State University; Florida State University; Florida State University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Organometal halide perovskites have recently emerged as a highly promising class of functional materials for a variety of applications. The exceptional structural tunability enables these materials to possess three- (3D), two- (2D), one- (1D), and zero-dimensional (0D) structures at the molecular level. Remarkable progress has been realized in the research of perovskites in recent years, focusing mainly on 3D and 2D structures but leaving low-dimensional 1D and 0D structures significantly underexplored. Here we offer our perspective on the most exciting developments in the low-dimensional organometal halide perovskites. Due to the strong quantum confinement and site isolation, 1D and 0D perovskites exhibit remarkable and useful properties that are significantly different from those of 3D and 2D perovskites. The excitement about the recent developments lies not only in the specific achievements but also in what these materials represent in terms of a new paradigm in materials design.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.7b00926

Chinese Library Classification Number:

Citation Information:

Organometal halide perovskites have recently emerged as a highly promising class of functional materials for a variety of applications. The exceptional structural tunability enables these materials to possess three- (3D), two- (2D), one- (1D), and zero-dimensional (0D) structures at the molecular level. Remarkable progress has been realized in the research of perovskites in recent years, focusing mainly on 3D and 2D structures but leaving low-dimensional 1D and 0D structures significantly underexplored. Here we offer our perspective on the most exciting developments in the low-dimensional organometal halide perovskites. Due to the strong quantum confinement and site isolation, 1D and 0D perovskites exhibit remarkable and useful properties that are significantly different from those of 3D and 2D perovskites. The excitement about the recent developments lies not only in the specific achievements but also in what these materials represent in terms of a new paradigm in materials design.

quote

GB/T 7714-2015 [1] Haoran Lin, Chenkun Zhou, Yu Tian, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.7b00926.
MLA [1] Haoran Lin, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.7b00926.
APA [1] Haoran Lin, Chenkun Zhou, Yu Tian, Theo Siegrist, & Biwu Ma. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.7b00926