daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Positive and Negative Aspects of Interfaces in Solid-State Batteries AITranslate

National Institute for Materials Science; National Institute for Materials Science; National Institute for Materials Science; National Institute for Materials Science; National Institute for Materials Science
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Solid-state lithium batteries are regarded as promising energy storage devices that meet the requirements for realizing a low-carbon society. Although solid-state batteries have been suffering from low power density, the power density has become comparable to or greater than that of liquid systems in a recently developed battery, which has been achieved not only by the high ionic conductivity of the used sulfide solid electrolyte. This Perspective presents anomalous transport properties appearing at the interfaces in solid-state batteries to highlight the importance of controlling the interface phenomena in achieving the high performance. The battery employs not only the highly conductive sulfide but also some oxides in spite of their low conductivity. LiNbO3 interposed to the cathode interface effectively reduces the cathode impedance by suppressing lithium depletion at the interface. Li4Ti5O12 used as the anode becomes a good conductor in its two-phase region because of enhanced transport properties at the phase boundaries.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.7b01105

Chinese Library Classification Number:

Citation Information:

Solid-state lithium batteries are regarded as promising energy storage devices that meet the requirements for realizing a low-carbon society. Although solid-state batteries have been suffering from low power density, the power density has become comparable to or greater than that of liquid systems in a recently developed battery, which has been achieved not only by the high ionic conductivity of the used sulfide solid electrolyte. This Perspective presents anomalous transport properties appearing at the interfaces in solid-state batteries to highlight the importance of controlling the interface phenomena in achieving the high performance. The battery employs not only the highly conductive sulfide but also some oxides in spite of their low conductivity. LiNbO3 interposed to the cathode interface effectively reduces the cathode impedance by suppressing lithium depletion at the interface. Li4Ti5O12 used as the anode becomes a good conductor in its two-phase region because of enhanced transport properties at the phase boundaries.

quote

GB/T 7714-2015 [1] Kazunori Takada, Takahisa Ohno, Narumi Ohta, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.7b01105.
MLA [1] Kazunori Takada, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.7b01105.
APA [1] Kazunori Takada, Takahisa Ohno, Narumi Ohta, Tsuyoshi Ohnishi, & Yoshinori Tanaka. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.7b01105
IEEE [1] Kazunori Takada, Takahisa Ohno, Narumi Ohta, Tsuyoshi Ohnishi, and Yoshinori Tanaka, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.7b01105.