Abstract AITranslate
Symmetric aqueous organic redox flow batteries (RFBs) are potentially an inexpensive, durable, and safe energy storage technology. Unlike normal asymmetric flow batteries, they are based on electrolytes that exist in at least three oxidation states and can undergo a minimum of two distinct redox processes. We compute the redox potentials of selected electrolytes, with the intent to understand how the interaction between the redox units affects the potentials. We find that electronic interaction between redox units and intramolecular hydrogen bonding can be exploited to tune the difference between the redox potentials, i.e., the theoretical voltage of the battery. The redox potentials can be further fine-tuned in either direction by adding substituents. Starting from these observations, we formulate a set of rules that will help in finding ideal candidates for symmetric RFBs.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.0c00028
Chinese Library Classification Number:
Citation Information:
Symmetric aqueous organic redox flow batteries (RFBs) are potentially an inexpensive, durable, and safe energy storage technology. Unlike normal asymmetric flow batteries, they are based on electrolytes that exist in at least three oxidation states and can undergo a minimum of two distinct redox processes. We compute the redox potentials of selected electrolytes, with the intent to understand how the interaction between the redox units affects the potentials. We find that electronic interaction between redox units and intramolecular hydrogen bonding can be exploited to tune the difference between the redox potentials, i.e., the theoretical voltage of the battery. The redox potentials can be further fine-tuned in either direction by adding substituents. Starting from these observations, we formulate a set of rules that will help in finding ideal candidates for symmetric RFBs.
quote
| GB/T 7714-2015 | [1] Rocco Peter Fornari, Murat Mesta, Johan Hjelm, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00028. |
| MLA | [1] Rocco Peter Fornari, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00028. |
| APA | [1] Rocco Peter Fornari, Murat Mesta, Johan Hjelm, Tejs Vegge, & Piotr de Silva. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00028 |
| IEEE | [1] Rocco Peter Fornari, Murat Mesta, Johan Hjelm, Tejs Vegge, and Piotr de Silva, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00028. |