daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Toward Phase Stability: Dion–Jacobson Layered Perovskite for Solar Cells AITranslate

BCMaterials, Basque Center for Materials;BCMaterials, Basque Center for Materials; Huazhong University of Science and Technology;BCMaterials, Basque Center for Materials
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Three-dimensional halide-based perovskites have emerged as promising semiconducting light harvesters for thin-film solar cell fabrication; however, their intrinsic instability under humidity restricts their potential commercialization. To address such challenges, the development of low-dimensional/layered Dion–Jacobson (DJ) phase perovskites has recently gained substantial attention due to their intriguing environmental stability and competitive power conversion efficiency. In this Review, we have screened and focused our investigation on the DJ phase in layered perovskites for solar cell fabrication, especially elucidation of the active role played by organic spacer cations. We also discuss the possible strategies that can be employed to further push the performance of DJ-based perovskite solar cells.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b02063

Chinese Library Classification Number:

Citation Information:

Three-dimensional halide-based perovskites have emerged as promising semiconducting light harvesters for thin-film solar cell fabrication; however, their intrinsic instability under humidity restricts their potential commercialization. To address such challenges, the development of low-dimensional/layered Dion–Jacobson (DJ) phase perovskites has recently gained substantial attention due to their intriguing environmental stability and competitive power conversion efficiency. In this Review, we have screened and focused our investigation on the DJ phase in layered perovskites for solar cell fabrication, especially elucidation of the active role played by organic spacer cations. We also discuss the possible strategies that can be employed to further push the performance of DJ-based perovskite solar cells.

quote

GB/T 7714-2015 [1] Peng Huang, Samrana Kazim, Mingkui Wang, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b02063.
MLA [1] Peng Huang, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b02063.
APA [1] Peng Huang, Samrana Kazim, Mingkui Wang, & Shahzada Ahmad. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b02063
IEEE [1] Peng Huang, Samrana Kazim, Mingkui Wang, and Shahzada Ahmad, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b02063.