Temperature-Dependent Solubility of Solid Electrolyte Interphase on Silicon Electrodes AITranslate

National Renewable Energy Laboratory;National Renewable Energy Laboratory;National Renewable Energy Laboratory;Colorado School of Mines;National Renewable Energy Laboratory;National Renewable Energy Laboratory; University of Colorado Boulder;National Renewable Energy Laboratory
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The lithium-ion batteries powering mass market electric vehicles must be capable of operating in a wide temperature range. Temperature variation has the potential to greatly affect the stability of the solid electrolyte interphase (SEI) responsible for mitigating capacity fade due to electrolyte decomposition in the lithium-ion battery. In this work, we investigate the solubility of the SEI on the silicon (Si) electrode, an alternative anode material to the conventional graphite electrode, at temperatures ranging from −10 to 50 °C. Through use of an electrochemical protocol with a high cathodic cutoff voltage, we measure the evolution of the SEI independently of competing Si mechanical stress. We correlate the electrochemical data with three-dimensional resistivity versus depth profiling as well as atomic force microscopy to show that SEI dissolution occurs at significantly faster rates at higher temperatures.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b02082

Chinese Library Classification Number:

Citation Information:

The lithium-ion batteries powering mass market electric vehicles must be capable of operating in a wide temperature range. Temperature variation has the potential to greatly affect the stability of the solid electrolyte interphase (SEI) responsible for mitigating capacity fade due to electrolyte decomposition in the lithium-ion battery. In this work, we investigate the solubility of the SEI on the silicon (Si) electrode, an alternative anode material to the conventional graphite electrode, at temperatures ranging from −10 to 50 °C. Through use of an electrochemical protocol with a high cathodic cutoff voltage, we measure the evolution of the SEI independently of competing Si mechanical stress. We correlate the electrochemical data with three-dimensional resistivity versus depth profiling as well as atomic force microscopy to show that SEI dissolution occurs at significantly faster rates at higher temperatures.

quote

GB/T 7714-2015 [1] Caleb Stetson, Yanli Yin, ChunSheng Jiang, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b02082.
MLA [1] Caleb Stetson, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b02082.
APA [1] Caleb Stetson, Yanli Yin, ChunSheng Jiang, Steven C. DeCaluwe, Mowafak AlJassim, Nathan R. Neale, Chunmei Ban, & Anthony Burrell. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b02082
IEEE [1] Caleb Stetson, Yanli Yin, ChunSheng Jiang, Steven C. DeCaluwe, Mowafak AlJassim, Nathan R. Neale, Chunmei Ban, and Anthony Burrell, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b02082.