Effect of Residual Chloride in FAPbI3 Film on Photovoltaic Performance and Stability of Perovskite Solar Cell AITranslate

Sungkyunkwan University; Sungkyunkwan University; Sungkyunkwan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Methylammonium chloride (MACl) has been used as an additive in a formamidinium lead iodide (FAPbI3) precursor solution for high-efficiency perovskite solar cells (PCSs), where the chloride ion is known to have a positive effect on photovoltaic performance. However, we have found that the residual chloride in the perovskite film has an adverse effect on the device stability. Here, we report an improved stability of PSCs by elimination of residual chloride via postheat-treatment (PHT). Removal of the residual MACl on the perovskite grain surface is accompanied by conversion of surface FAPbI3 to PbI2. Compared with the control perovskite film, the PHT-induced perovskite film shows a longer charge carrier lifetime, which is responsible for an increase in the reverse scanned power conversion efficiency from 21.17% to 23.20%. Moreover, long-term stability tested under humid air conditions for over 1000 h shows that the chloride-removed perovskite film is much more stable than the control film with residual chloride.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00568

Chinese Library Classification Number:

Citation Information:

Methylammonium chloride (MACl) has been used as an additive in a formamidinium lead iodide (FAPbI3) precursor solution for high-efficiency perovskite solar cells (PCSs), where the chloride ion is known to have a positive effect on photovoltaic performance. However, we have found that the residual chloride in the perovskite film has an adverse effect on the device stability. Here, we report an improved stability of PSCs by elimination of residual chloride via postheat-treatment (PHT). Removal of the residual MACl on the perovskite grain surface is accompanied by conversion of surface FAPbI3 to PbI2. Compared with the control perovskite film, the PHT-induced perovskite film shows a longer charge carrier lifetime, which is responsible for an increase in the reverse scanned power conversion efficiency from 21.17% to 23.20%. Moreover, long-term stability tested under humid air conditions for over 1000 h shows that the chloride-removed perovskite film is much more stable than the control film with residual chloride.

quote

GB/T 7714-2015 [1] DongHo Kang, SangUk Lee, NamGyu Park. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00568.
MLA [1] DongHo Kang, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00568.
APA [1] DongHo Kang, SangUk Lee, & NamGyu Park. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00568
IEEE [1] DongHo Kang, SangUk Lee, and NamGyu Park, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00568.