daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Carrier Cooling in Lead Halide Perovskites: A Perspective on Hot Carrier Solar Cells AITranslate

Lund University; Technical University of Denmark; Technical University of Denmark; Lund University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The concept of hot carrier solar cells (HCSCs) has been proposed as a promising yet elusive path toward high-performance photovoltaics (PV), capable of surpassing the Shockley–Queisser limit by recycling energy that would otherwise be lost during thermalization. Lead halide perovskites (LHPs) have emerged as highly promising materials for PV applications. The reports of slow hot carrier (HC) cooling in these materials have ignited discussions of their potential in realizing HCSCs. Here we summarize the key findings regarding HC dynamics in LHPs, as revealed by numerous studies using advanced time-resolved spectroscopies. We also emphasize the interconnected mechanisms involved in HC cooling. In addition, we discuss the influence of nanostructuring on HC cooling dynamics in LHPs and suggest that two-dimensional LHPs, with their inherent quantum well structure, might exhibit modified phononic features and altered carrier–phonon coupling strength. We conclude by critically discussing the prospects for HCSCs, taking into account our current understanding of HC cooling and excitation conditions under sunlight.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c02359

Chinese Library Classification Number:

Citation Information:

The concept of hot carrier solar cells (HCSCs) has been proposed as a promising yet elusive path toward high-performance photovoltaics (PV), capable of surpassing the Shockley–Queisser limit by recycling energy that would otherwise be lost during thermalization. Lead halide perovskites (LHPs) have emerged as highly promising materials for PV applications. The reports of slow hot carrier (HC) cooling in these materials have ignited discussions of their potential in realizing HCSCs. Here we summarize the key findings regarding HC dynamics in LHPs, as revealed by numerous studies using advanced time-resolved spectroscopies. We also emphasize the interconnected mechanisms involved in HC cooling. In addition, we discuss the influence of nanostructuring on HC cooling dynamics in LHPs and suggest that two-dimensional LHPs, with their inherent quantum well structure, might exhibit modified phononic features and altered carrier–phonon coupling strength. We conclude by critically discussing the prospects for HCSCs, taking into account our current understanding of HC cooling and excitation conditions under sunlight.

quote

GB/T 7714-2015 [1] Weihua Lin, Sophie E. Canton, Kaibo Zheng, et al. ACS Energy Letters, 2024(9). DOI:10.1021/acsenergylett.3c02359.
MLA [1] Weihua Lin, et al., ACS Energy Letters, no. 9, 2024, https://doi.org/10.1021/acsenergylett.3c02359.
APA [1] Weihua Lin, Sophie E. Canton, Kaibo Zheng, & Tõnu Pullerits. (2024). ACS Energy Letters(9). https://doi.org/10.1021/acsenergylett.3c02359
IEEE [1] Weihua Lin, Sophie E. Canton, Kaibo Zheng, and Tõnu Pullerits, ACS Energy Letters, no. 9, 2024, doi: 10.1021/acsenergylett.3c02359.