Dielectric Engineering of 2D Organic–Inorganic Hybrid Perovskites AITranslate

Nanjing University of Posts and Telecommunications; Nanjing University of Posts and Telecommunications; Nanjing University of Posts and Telecommunications; Nanjing University of Posts and Telecommunications; Nanjing University of Posts and Telecommunications; Nanjing University of Posts and Telecommunications; Nanjing University of Posts and Telecommunications; Nanjing University of Posts and Telecommunications
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Manipulating excitons in semiconductors has driven the evolution of today’s optoelectronic and photovoltaic devices. Engineering the dielectric constant, a key parameter that is highly associated with the Coulomb force of excitons, has recently emerged as a fresh avenue to regulate excitons from the root. Unlike three-dimensional (3D) bulk semiconductors featuring uniformly distributed dielectric constants, the dielectric constants of two-dimensional (2D) layered semiconductors exhibit spatial variability. Particularly, organic–inorganic hybrid perovskites (OIHPs) assembled with alternating organic and inorganic layers show a cyclic variation in the dielectric property, which substantially impacts exciton dynamics, including recombination and separation, offering an opportunity for the regulation of exciton-related physical attributes by dielectric engineering and the cutting-edge applications thereof. This Review documents the recent advances in the rational design of organic and inorganic constituents of 2D OIHPs for dielectric engineering. We show that dielectrically engineered OIHPs are pivotal in driving the advancements in optoelectrical and photovoltaic applications.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c02069

Chinese Library Classification Number:

Citation Information:

Manipulating excitons in semiconductors has driven the evolution of today’s optoelectronic and photovoltaic devices. Engineering the dielectric constant, a key parameter that is highly associated with the Coulomb force of excitons, has recently emerged as a fresh avenue to regulate excitons from the root. Unlike three-dimensional (3D) bulk semiconductors featuring uniformly distributed dielectric constants, the dielectric constants of two-dimensional (2D) layered semiconductors exhibit spatial variability. Particularly, organic–inorganic hybrid perovskites (OIHPs) assembled with alternating organic and inorganic layers show a cyclic variation in the dielectric property, which substantially impacts exciton dynamics, including recombination and separation, offering an opportunity for the regulation of exciton-related physical attributes by dielectric engineering and the cutting-edge applications thereof. This Review documents the recent advances in the rational design of organic and inorganic constituents of 2D OIHPs for dielectric engineering. We show that dielectrically engineered OIHPs are pivotal in driving the advancements in optoelectrical and photovoltaic applications.

quote

GB/T 7714-2015 [1] Bing Chen, Rongrong Yu, Guansheng Xing, et al. ACS Energy Letters, 2024(9). DOI:10.1021/acsenergylett.3c02069.
MLA [1] Bing Chen, et al., ACS Energy Letters, no. 9, 2024, https://doi.org/10.1021/acsenergylett.3c02069.
APA [1] Bing Chen, Rongrong Yu, Guansheng Xing, Yulong Wang, Wenlong Wang, Ya Chen, Xiuwen Xu, & Qiang Zhao. (2024). ACS Energy Letters(9). https://doi.org/10.1021/acsenergylett.3c02069
IEEE [1] Bing Chen, Rongrong Yu, Guansheng Xing, Yulong Wang, Wenlong Wang, Ya Chen, Xiuwen Xu, and Qiang Zhao, ACS Energy Letters, no. 9, 2024, doi: 10.1021/acsenergylett.3c02069.