Solution-Processed Cu2S Photocathodes for Photoelectrochemical Water Splitting AITranslate
Abstract AITranslate
Cu2S has been regarded as a promising solar energy conversion material because of its favorable visible light absorption and earth abundance. Here, we present an indirect preparation method via a solution-processed ion exchange reaction to synthesize stoichiometric Cu2S films with high photoactivity. In addition, we developed a chemical bath deposition method to fabricate CdS buffer layers on Cu2S by adding a reducing agent in the precursor solution, avoiding oxidation of Cu2S. After being coated with the TiO2 protection layer and the RuOx hydrogen evolution catalyst, the Cu2S photoelectrode delivers a photocurrent density of 7.0 mA cm–2 at −0.3 V vs RHE and an onset potential of 0.48 V vs RHE under AM 1.5G simulated sunlight illumination for solar driven water reduction. To our knowledge, this is the first time that Cu2S has been used for solar hydrogen evolution with encouraging performance, which will stimulate further studies on Cu-based photocathodes.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.7b01326
Chinese Library Classification Number:
Citation Information:
Cu2S has been regarded as a promising solar energy conversion material because of its favorable visible light absorption and earth abundance. Here, we present an indirect preparation method via a solution-processed ion exchange reaction to synthesize stoichiometric Cu2S films with high photoactivity. In addition, we developed a chemical bath deposition method to fabricate CdS buffer layers on Cu2S by adding a reducing agent in the precursor solution, avoiding oxidation of Cu2S. After being coated with the TiO2 protection layer and the RuOx hydrogen evolution catalyst, the Cu2S photoelectrode delivers a photocurrent density of 7.0 mA cm–2 at −0.3 V vs RHE and an onset potential of 0.48 V vs RHE under AM 1.5G simulated sunlight illumination for solar driven water reduction. To our knowledge, this is the first time that Cu2S has been used for solar hydrogen evolution with encouraging performance, which will stimulate further studies on Cu-based photocathodes.
quote
| GB/T 7714-2015 | [1] YuXiang Yu, Linfeng Pan, MinKyu Son, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.7b01326. |
| MLA | [1] YuXiang Yu, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.7b01326. |
| APA | [1] YuXiang Yu, Linfeng Pan, MinKyu Son, Matthew T. Mayer, WeiDe Zhang, Anders Hagfeldt, Jingshan Luo, & Michael Grätzel. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.7b01326 |
| IEEE | [1] YuXiang Yu, Linfeng Pan, MinKyu Son, Matthew T. Mayer, WeiDe Zhang, Anders Hagfeldt, Jingshan Luo, and Michael Grätzel, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.7b01326. |