Efficient and Selective Photocatalytic Oxidation of Benzylic Alcohols with Hybrid Organic–Inorganic Perovskite Materials AITranslate

Department of Microbial and Molecular Systems, Centre for Surface Chemistry and Catalysis (COK);Department of Chemistry, Faculty of Sciences;Department of Chemistry, Faculty of Sciences;Department of Chemistry, Faculty of Sciences; Fuzhou University;Department of Microbial and Molecular Systems, Centre for Surface Chemistry and Catalysis (COK);Department of Microbial and Molecular Systems, Centre for Surface Chemistry and Catalysis (COK);Department of Chemistry, Faculty of Sciences; Fuzhou University;Department of Chemistry, Faculty of Sciences;Department of Chemistry, Faculty of Sciences;Department of Microbial and Molecular Systems, Centre for Surface Chemistry and Catalysis (COK);Department of Microbial and Molecular Systems, Centre for Surface Chemistry and Catalysis (COK)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The impressive optoelectronic performance and low production cost of metal halide perovskites have inspired applications well beyond efficient solar cells. Herein, we widen the materials engineering options available for the efficient and selective photocatalytic oxidation of benzylic alcohols, an industrially significant reaction, using formamidinium lead bromide (FAPbBr3) and other perovskite-based materials. The best performance was obtained using a FAPbBr3/TiO2 hybrid photocatalyst under simulated solar illumination. Detailed optical studies reveal the synergetic photophysical pathways arising in FAPbBr3/TiO2 composites. An experimentally supported model rationalizing the large conversion enhancement over the pure constituents shows that this strategy offers new prospects for metal halide perovskites in photocatalytic applications.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b00131

Chinese Library Classification Number:

Citation Information:

The impressive optoelectronic performance and low production cost of metal halide perovskites have inspired applications well beyond efficient solar cells. Herein, we widen the materials engineering options available for the efficient and selective photocatalytic oxidation of benzylic alcohols, an industrially significant reaction, using formamidinium lead bromide (FAPbBr3) and other perovskite-based materials. The best performance was obtained using a FAPbBr3/TiO2 hybrid photocatalyst under simulated solar illumination. Detailed optical studies reveal the synergetic photophysical pathways arising in FAPbBr3/TiO2 composites. An experimentally supported model rationalizing the large conversion enhancement over the pure constituents shows that this strategy offers new prospects for metal halide perovskites in photocatalytic applications.

quote

GB/T 7714-2015 [1] Haowei Huang, Haifeng Yuan, Kris P. F. Janssen, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00131.
MLA [1] Haowei Huang, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00131.
APA [1] Haowei Huang, Haifeng Yuan, Kris P. F. Janssen, Guillermo SolísFernández, Ying Wang, Collin Y. X. Tan, Dries Jonckheere, Elke Debroye, Jinlin Long, Jelle Hendrix, Johan Hofkens, Julian A. Steele, & Maarten B. J. Roeffaers. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00131
IEEE [1] Haowei Huang, Haifeng Yuan, Kris P. F. Janssen, Guillermo SolísFernández, Ying Wang, Collin Y. X. Tan, Dries Jonckheere, Elke Debroye, Jinlin Long, Jelle Hendrix, Johan Hofkens, Julian A. Steele, and Maarten B. J. Roeffaers, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00131.