daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Understanding the Surface Regeneration and Reactivity of Garnet Solid-State Electrolytes AITranslate

University of Cambridge; University of Cambridge; University of Cambridge;Diamond Light Source, Harwell Science and Innovation Campus;Fakultät Physik/DELTA, Technische Universität Dortmund;Fakultät Physik/DELTA, Technische Universität Dortmund;Diamond Light Source, Harwell Science and Innovation Campus; University of Cambridge
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Garnet solid-electrolyte-based Li-metal batteries can be used in energy storage devices with high energy densities and thermal stability. However, the tendency of garnets to form lithium hydroxide and carbonate on the surface in an ambient atmosphere poses significant processing challenges. In this work, the decomposition of surface layers under various gas environments is studied by using two surface-sensitive techniques, near-ambient-pressure X-ray photoelectron spectroscopy and grazing incidence X-ray diffraction. It is found that heating to 500 °C under an oxygen atmosphere (of 1 mbar and above) leads to a clean garnet surface, whereas low oxygen partial pressures (i.e., in argon or vacuum) lead to additional graphitic carbon deposits. The clean surface of garnets reacts directly with moisture and carbon dioxide below 400 and 500 °C, respectively. This suggests that additional CO2 concentration controls are needed for the handling of garnets. By heating under O2 along with avoiding H2O and CO2, symmetric cells with less than 10 Ωcm2 interface resistance are prepared without the use of any interlayers; plating currents of >1 mA cm–2 without dendrite initiation are demonstrated.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c01042

Chinese Library Classification Number:

Citation Information:

Garnet solid-electrolyte-based Li-metal batteries can be used in energy storage devices with high energy densities and thermal stability. However, the tendency of garnets to form lithium hydroxide and carbonate on the surface in an ambient atmosphere poses significant processing challenges. In this work, the decomposition of surface layers under various gas environments is studied by using two surface-sensitive techniques, near-ambient-pressure X-ray photoelectron spectroscopy and grazing incidence X-ray diffraction. It is found that heating to 500 °C under an oxygen atmosphere (of 1 mbar and above) leads to a clean garnet surface, whereas low oxygen partial pressures (i.e., in argon or vacuum) lead to additional graphitic carbon deposits. The clean surface of garnets reacts directly with moisture and carbon dioxide below 400 and 500 °C, respectively. This suggests that additional CO2 concentration controls are needed for the handling of garnets. By heating under O2 along with avoiding H2O and CO2, symmetric cells with less than 10 Ωcm2 interface resistance are prepared without the use of any interlayers; plating currents of >1 mA cm–2 without dendrite initiation are demonstrated.

quote

GB/T 7714-2015 [1] Sundeep Vema, Farheen N. Sayed, Supreeth Nagendran, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01042.
MLA [1] Sundeep Vema, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01042.
APA [1] Sundeep Vema, Farheen N. Sayed, Supreeth Nagendran, Burcu Karagoz, Christian Sternemann, Michael Paulus, Georg Held, & Clare P. Grey. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01042
IEEE [1] Sundeep Vema, Farheen N. Sayed, Supreeth Nagendran, Burcu Karagoz, Christian Sternemann, Michael Paulus, Georg Held, and Clare P. Grey, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c01042.