Customized Electrolyte and Host Structures Enabling High-Energy-Density Anode-Free Potassium–Metal Batteries AITranslate

Huazhong University of Science and Technology; Huazhong University of Science and Technology;Suzhou Laboratory;GuSu Laboratory of Materials; Huazhong University of Science and Technology; Huazhong University of Science and Technology; Huazhong University of Science and Technology; Huazhong University of Science and Technology; Huazhong University of Science and Technology; Huazhong University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Potassium shows great potential to replace lithium in energy storage for its high abundance and comparable energy density. However, issues including an unstable interphase, dendrite growth, and volume change restrict the development of potassium metal batteries, and so far, there is no single cure that works once and for all. Here an anode-free potassium metal battery is demonstrated by introducing a customized electrolyte and host structures that simultaneously promote efficiency, reversibility, and energy density. First, a diluted high-concentration electrolyte with fast kinetics and high stability triggers an inorganic-rich durable interphase. Meanwhile, a carbonaceous host containing narrowly distributed mesopores (MCNF) favors reduced surface area but enough inner space. Together, they achieve a high average Coulombic efficiency (CE) of 99.3% and an initial CE of 95.9% at 3 mA cm–2–3 mA h cm–2. Anode-free MCNF||Prussian blue (PB) potassium cells are delivered with 100 reversible cycles and a high energy density of 362 W h kg–1.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c01067

Chinese Library Classification Number:

Citation Information:

Potassium shows great potential to replace lithium in energy storage for its high abundance and comparable energy density. However, issues including an unstable interphase, dendrite growth, and volume change restrict the development of potassium metal batteries, and so far, there is no single cure that works once and for all. Here an anode-free potassium metal battery is demonstrated by introducing a customized electrolyte and host structures that simultaneously promote efficiency, reversibility, and energy density. First, a diluted high-concentration electrolyte with fast kinetics and high stability triggers an inorganic-rich durable interphase. Meanwhile, a carbonaceous host containing narrowly distributed mesopores (MCNF) favors reduced surface area but enough inner space. Together, they achieve a high average Coulombic efficiency (CE) of 99.3% and an initial CE of 95.9% at 3 mA cm–2–3 mA h cm–2. Anode-free MCNF||Prussian blue (PB) potassium cells are delivered with 100 reversible cycles and a high energy density of 362 W h kg–1.

quote

GB/T 7714-2015 [1] Siwu Li, Haolin Zhu, Chenkai Gu, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01067.
MLA [1] Siwu Li, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01067.
APA [1] Siwu Li, Haolin Zhu, Chenkai Gu, Fenfen Ma, Wei Zhong, Mengchuang Liu, Han Zhang, Ziqi Zeng, Shijie Cheng, & Jia Xie. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01067
IEEE [1] Siwu Li, Haolin Zhu, Chenkai Gu, Fenfen Ma, Wei Zhong, Mengchuang Liu, Han Zhang, Ziqi Zeng, Shijie Cheng, and Jia Xie, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c01067.