The Effect of Pendent Groups upon Flexibility in Coordination Networks with Square Lattice Topology AITranslate
Abstract AITranslate
Gas or vapor-induced phase transformations in flexible coordination networks (CNs) offer the potential to exceed the performance of their rigid counterparts for separation and storage applications. However, whereas ligand modification has been used to alter the properties of such stimulus-responsive materials, they remain understudied compared with their rigid counterparts. Here, we report that a family of Zn2+ CNs with square lattice (sql) topology, differing only through the substituents attached to a linker, exhibit variable flexibility. Structural and CO2 sorption studies on the sql networks, [Zn(5-Ria)(bphy)]n, ia = isophthalic acid, bphy = 1,2-bis(pyridin-4-yl)hydrazine, R = −CH3, −OCH3, −C(CH3)3, -N═N-Ph, and -N═N-Ph(CH3)2, 2–6, respectively, revealed that the substituent moieties influenced both structural and gas sorption properties. Whereas 2–3 exhibited rigidity, 4, 5, and 6 exhibited reversible transformation from small pore to large pore phases. Overall, the insight into the profound effect of pendent moieties of linkers upon phase transformations in this family of layered CNs should be transferable to other CN classes.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.3c00565
Chinese Library Classification Number:
Citation Information:
Gas or vapor-induced phase transformations in flexible coordination networks (CNs) offer the potential to exceed the performance of their rigid counterparts for separation and storage applications. However, whereas ligand modification has been used to alter the properties of such stimulus-responsive materials, they remain understudied compared with their rigid counterparts. Here, we report that a family of Zn2+ CNs with square lattice (sql) topology, differing only through the substituents attached to a linker, exhibit variable flexibility. Structural and CO2 sorption studies on the sql networks, [Zn(5-Ria)(bphy)]n, ia = isophthalic acid, bphy = 1,2-bis(pyridin-4-yl)hydrazine, R = −CH3, −OCH3, −C(CH3)3, -N═N-Ph, and -N═N-Ph(CH3)2, 2–6, respectively, revealed that the substituent moieties influenced both structural and gas sorption properties. Whereas 2–3 exhibited rigidity, 4, 5, and 6 exhibited reversible transformation from small pore to large pore phases. Overall, the insight into the profound effect of pendent moieties of linkers upon phase transformations in this family of layered CNs should be transferable to other CN classes.
quote
| GB/T 7714-2015 | [1] Xia Li, Debobroto Sensharma, Kyriaki Koupepidou, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00565. |
| MLA | [1] Xia Li, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00565. |
| APA | [1] Xia Li, Debobroto Sensharma, Kyriaki Koupepidou, XiangJing Kong, & Michael J. Zaworotko. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00565 |
| IEEE | [1] Xia Li, Debobroto Sensharma, Kyriaki Koupepidou, XiangJing Kong, and Michael J. Zaworotko, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00565. |