Self-Rotating Spherical Evaporator Based on Hydrogel and Black Titanium Oxide for Continuous Desalination of Seawater AITranslate

China Jiliang University; China Jiliang University; China Jiliang University; China Jiliang University; China Jiliang University;Songshan Lake Materials Laboratory; The Hong Kong Polytechnic University; China Jiliang University; China Jiliang University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Solar interfacial water evaporation technology has shown great promise for seawater desalination and wastewater treatment. However, the deposition of salt crystals on the evaporator surface restrains the evaporation rate, which will affect further development of this technology. In this work, a spherical polystyrene foam was utilized as the material support, the surface of which was coated with photothermal materials for evaporator fabrication. The employing of well-prepared black Ti4O7 as a photothermal coating greatly improve the sunlight absorption of the surface, and the mixing of sodium alginate can achieve a hydrophilic effect. This unique coordination not only increases the evaporation rate of the spherical evaporator (2.46 kg m–2 h–1), but also performs well in water purification. The spherical design allows the evaporator to periodically clean the salt deposits on the evaporator surface through self-rotation, which provides a promising way to deal with the problem of salt deposition in evaporators in the future.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c00761

Chinese Library Classification Number:

Citation Information:

Solar interfacial water evaporation technology has shown great promise for seawater desalination and wastewater treatment. However, the deposition of salt crystals on the evaporator surface restrains the evaporation rate, which will affect further development of this technology. In this work, a spherical polystyrene foam was utilized as the material support, the surface of which was coated with photothermal materials for evaporator fabrication. The employing of well-prepared black Ti4O7 as a photothermal coating greatly improve the sunlight absorption of the surface, and the mixing of sodium alginate can achieve a hydrophilic effect. This unique coordination not only increases the evaporation rate of the spherical evaporator (2.46 kg m–2 h–1), but also performs well in water purification. The spherical design allows the evaporator to periodically clean the salt deposits on the evaporator surface through self-rotation, which provides a promising way to deal with the problem of salt deposition in evaporators in the future.

quote

GB/T 7714-2015 [1] Yumeng Ge, Zewen Su, Le Wang, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00761.
MLA [1] Yumeng Ge, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00761.
APA [1] Yumeng Ge, Zewen Su, Le Wang, Congcong Wang, Peiqing Cai, Shenghuang Lin, Yuan Liu, Shiqing Xu, & Gongxun Bai. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00761
IEEE [1] Yumeng Ge, Zewen Su, Le Wang, Congcong Wang, Peiqing Cai, Shenghuang Lin, Yuan Liu, Shiqing Xu, and Gongxun Bai, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00761.