Coulometric detector based on carbon felt AITranslate

Charles University;Charles University;Charles University;Charles University;Charles University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Carbon felt was used as the working material in a simple high-conversion electrochemical detector. Influence of the main parameters on the detection was tested using flow injection analysis with standard redox systems. Convenient properties of the detector include high conversion rate, sufficient repeatability of both injection and carbon felt replacement, and linear concentration dependences. Practical applicability of the newly developed detector was verified by the development of methods for HPLC determination of four synthetic phenolic antioxidants in edible oil sample. Graphical abstract Download : Download high-res image (81KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2017.09.012

Chinese Library Classification Number:

Citation Information:

Carbon felt was used as the working material in a simple high-conversion electrochemical detector. Influence of the main parameters on the detection was tested using flow injection analysis with standard redox systems. Convenient properties of the detector include high conversion rate, sufficient repeatability of both injection and carbon felt replacement, and linear concentration dependences. Practical applicability of the newly developed detector was verified by the development of methods for HPLC determination of four synthetic phenolic antioxidants in edible oil sample. Graphical abstract Download : Download high-res image (81KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Hana Dejmková, Martin Baroch, Markéta Krejčová, et al. Applied Materials Today, 2017(9). DOI:10.1016/j.apmt.2017.09.012.
MLA [1] Hana Dejmková, et al., Applied Materials Today, no. 9, 2017, https://doi.org/10.1016/j.apmt.2017.09.012.
APA [1] Hana Dejmková, Martin Baroch, Markéta Krejčová, Jiří Barek, & Jiří Zima. (2017). Applied Materials Today(9). https://doi.org/10.1016/j.apmt.2017.09.012
IEEE [1] Hana Dejmková, Martin Baroch, Markéta Krejčová, Jiří Barek, and Jiří Zima, Applied Materials Today, no. 9, 2017, doi: 10.1016/j.apmt.2017.09.012.