Polymer-assisted deposition of SrTiO3 film as cathode buffer layer in inverted polymer solar cells AITranslate

New Mexico State University; New Mexico State University; University of New Mexico; New Mexico State University; University of New Mexico; New Mexico State University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Polymer-assisted deposition (PAD) method has been employed to prepare SrTiO3(STO) films on ITO substrates, which have been applied as cathode buffer layer in inverted polymer solar cells. ZnO and TiO2 films on ITO glass were also prepared via PAD and have been utilized as cathode buffer layers in the inverted polymer solar cells for comparison, which show better efficiency than those using ZnO and TiO2 as interfacial layers prepared through other methods. The power conversion efficiency (PCE) of ∼3.5% was achieved with STO as the cathode buffer layer as well as MoO3 as the anode buffer layer, which is comparable to that with ZnO and TiO2 prepared using the same method as cathode buffer layers. Our findings indicate that STO has the potential to be a candidate as interfacial layers in solar cell devices. Graphical abstract Download : Download high-res image (134KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2017.09.004

Chinese Library Classification Number:

Citation Information:

Polymer-assisted deposition (PAD) method has been employed to prepare SrTiO3(STO) films on ITO substrates, which have been applied as cathode buffer layer in inverted polymer solar cells. ZnO and TiO2 films on ITO glass were also prepared via PAD and have been utilized as cathode buffer layers in the inverted polymer solar cells for comparison, which show better efficiency than those using ZnO and TiO2 as interfacial layers prepared through other methods. The power conversion efficiency (PCE) of ∼3.5% was achieved with STO as the cathode buffer layer as well as MoO3 as the anode buffer layer, which is comparable to that with ZnO and TiO2 prepared using the same method as cathode buffer layers. Our findings indicate that STO has the potential to be a candidate as interfacial layers in solar cell devices. Graphical abstract Download : Download high-res image (134KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Haizhen Wang, Brian Patterson, Jianzhong Yang, et al. Applied Materials Today, 2017(9). DOI:10.1016/j.apmt.2017.09.004.
MLA [1] Haizhen Wang, et al., Applied Materials Today, no. 9, 2017, https://doi.org/10.1016/j.apmt.2017.09.004.
APA [1] Haizhen Wang, Brian Patterson, Jianzhong Yang, Di Huang, Yang Qin, & Hongmei Luo. (2017). Applied Materials Today(9). https://doi.org/10.1016/j.apmt.2017.09.004
IEEE [1] Haizhen Wang, Brian Patterson, Jianzhong Yang, Di Huang, Yang Qin, and Hongmei Luo, Applied Materials Today, no. 9, 2017, doi: 10.1016/j.apmt.2017.09.004.