Fast Analytics of High-Impact Polypropylene (HIPP) AITranslate
Abstract AITranslate
High-impact polypropylenes (HIPPs) are complex blends, featuring a crystalline isotactic polypropylene matrix and a dispersed phase consisting of an amorphous ethylene/propylene copolymer (EPR). The relative amount of EPR and its composition heavily affect the application properties of the material and need to be accurately controlled. Standard analytical methods are time- and labor-intensive and require considerable amounts of sample and of a toxic solvent, xylene. Here, we introduce an analytical approach to HIPP characterization based on crystallization elution fractionation. The approach is fast, can be operated on just a few mg of sample, and does not require sophisticated and expensive techniques.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c00810
Chinese Library Classification Number:
Citation Information:
High-impact polypropylenes (HIPPs) are complex blends, featuring a crystalline isotactic polypropylene matrix and a dispersed phase consisting of an amorphous ethylene/propylene copolymer (EPR). The relative amount of EPR and its composition heavily affect the application properties of the material and need to be accurately controlled. Standard analytical methods are time- and labor-intensive and require considerable amounts of sample and of a toxic solvent, xylene. Here, we introduce an analytical approach to HIPP characterization based on crystallization elution fractionation. The approach is fast, can be operated on just a few mg of sample, and does not require sophisticated and expensive techniques.
quote
| GB/T 7714-2015 | [1] Giuseppe Antinucci, Andrea Pucciarelli, Antonio Vittoria, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00810. |
| MLA | [1] Giuseppe Antinucci, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00810. |
| APA | [1] Giuseppe Antinucci, Andrea Pucciarelli, Antonio Vittoria, Francesco Zaccaria, Gaia Urciuoli, Christian Ehm, Felicia Daniela Cannavacciuolo, Roberta Cipullo, & Vincenzo Busico. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00810 |
| IEEE | [1] Giuseppe Antinucci, Andrea Pucciarelli, Antonio Vittoria, Francesco Zaccaria, Gaia Urciuoli, Christian Ehm, Felicia Daniela Cannavacciuolo, Roberta Cipullo, and Vincenzo Busico, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00810. keywords: {Impact copolymer;highimpact polypropylene;crystallization elution fractionation technique;polypropylene;polyolefin;Show More} |