In the last decades, water pollution from different industries has been one of the largest environmental issues. Many efforts have been made to develop technologies to remove toxic pollutants from the contaminated waters, which are direct threats to the aquatic environment and human health. Among different technologies, heterogeneous catalysis has shown to be very effective for water purification. The main issue regarding this method is the water recovery after the treatment, which is a very expensive and laborious procedure but can be addressed by the immobilization of photocatalytic particles on the support material. Here, we present efficient and green technology for water purification based on ZnO/SnO2-poly(methyl methacrylate) (PMMA) nanocomposite foils utilizing superior photocatalytic properties of coupled ZnO and SnO2 photocatalysts. We investigated the influence of the ZnO/SnO2 nanoparticle concentration on the removal efficiency of methylene blue dye and found exceptional removal efficiency for even very low ZnO/SnO2 nanoparticle loadings. The investigated foils were found to be highly reusable, with no change in performance after five successive usages. The composition, optical properties, surface morphology, and surface roughness of the foils were characterized by X-ray diffraction, UV–vis spectroscopy, scanning electron microscopy, and atomic force microscopy. The thermal measurements performed with differential scanning calorimetry suggested the reinforcement effect of ZnO/SnO2 nanoparticles on the PMMA matrix, which is essential for practical applications of the foils.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c00396
Chinese Library Classification Number:
Citation Information:
In the last decades, water pollution from different industries has been one of the largest environmental issues. Many efforts have been made to develop technologies to remove toxic pollutants from the contaminated waters, which are direct threats to the aquatic environment and human health. Among different technologies, heterogeneous catalysis has shown to be very effective for water purification. The main issue regarding this method is the water recovery after the treatment, which is a very expensive and laborious procedure but can be addressed by the immobilization of photocatalytic particles on the support material. Here, we present efficient and green technology for water purification based on ZnO/SnO2-poly(methyl methacrylate) (PMMA) nanocomposite foils utilizing superior photocatalytic properties of coupled ZnO and SnO2 photocatalysts. We investigated the influence of the ZnO/SnO2 nanoparticle concentration on the removal efficiency of methylene blue dye and found exceptional removal efficiency for even very low ZnO/SnO2 nanoparticle loadings. The investigated foils were found to be highly reusable, with no change in performance after five successive usages. The composition, optical properties, surface morphology, and surface roughness of the foils were characterized by X-ray diffraction, UV–vis spectroscopy, scanning electron microscopy, and atomic force microscopy. The thermal measurements performed with differential scanning calorimetry suggested the reinforcement effect of ZnO/SnO2 nanoparticles on the PMMA matrix, which is essential for practical applications of the foils.
quote
| GB/T 7714-2015 | [1] Nevena Ćelić, Nemanja Banić, Ivana Jagodić, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00396. |
| MLA | [1] Nevena Ćelić, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00396. |
| APA | [1] Nevena Ćelić, Nemanja Banić, Ivana Jagodić, Roman Yatskiv, Jan Vaniš, Goran Štrbac, & Svetlana LukićPetrović. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00396 |
| IEEE | [1] Nevena Ćelić, Nemanja Banić, Ivana Jagodić, Roman Yatskiv, Jan Vaniš, Goran Štrbac, and Svetlana LukićPetrović, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00396. keywords: {ZnO/SnO2 nanoparticles;PMMA nanocomposites;polymers;photocatalysis;water treatment} |