Solventless Polymer-Grafted Mesh for Rapid and Efficient Oil–Water Separation AITranslate

Oklahoma State University; Oklahoma State University; Oklahoma State University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We report a solventless bilayer strategy for grafting hydrophilic poly(methacrylic acid) (PMAA) onto metal meshes. The bilayer nanocoating consisted of ultrathin PMAA brushes grafted onto a highly crosslinked primer that binds to each mesh wire. The enrichment of hydrophilic functionalities on the PMAA-grafted mesh surface improved the surface hydration and underwater oil repellency over the PMAA-crosslinked mesh, which contributed to the formation and stabilization of continuous water films between mesh wires to reject oil penetration in repeated uses. The vapor-based nanocoating process maximized the retention of pore openings for high-flux oil–water separation. The retained permeability, together with the enhanced oil repellency, enabled the PMAA-grafted mesh to achieve excellent gravity-driven oil–water separation, with an oil rejection rate higher than 99%, water flux exceeding 50,000 L m–2 h–1, and flux decay less than 3% after 20 cycles of reuse. More importantly, the PMAA-grafted mesh preserved high separation efficiency and flux stability under conditions of high salinity and extreme pH.

KeyWords AITranslate

grafting vapor deposition underwater superoleophobicity oil−water separation high flux
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00399

Chinese Library Classification Number:

Citation Information:

We report a solventless bilayer strategy for grafting hydrophilic poly(methacrylic acid) (PMAA) onto metal meshes. The bilayer nanocoating consisted of ultrathin PMAA brushes grafted onto a highly crosslinked primer that binds to each mesh wire. The enrichment of hydrophilic functionalities on the PMAA-grafted mesh surface improved the surface hydration and underwater oil repellency over the PMAA-crosslinked mesh, which contributed to the formation and stabilization of continuous water films between mesh wires to reject oil penetration in repeated uses. The vapor-based nanocoating process maximized the retention of pore openings for high-flux oil–water separation. The retained permeability, together with the enhanced oil repellency, enabled the PMAA-grafted mesh to achieve excellent gravity-driven oil–water separation, with an oil rejection rate higher than 99%, water flux exceeding 50,000 L m–2 h–1, and flux decay less than 3% after 20 cycles of reuse. More importantly, the PMAA-grafted mesh preserved high separation efficiency and flux stability under conditions of high salinity and extreme pH.

quote

GB/T 7714-2015 [1] Chengqian Huang, Mengfan Zhu, Yu Mao. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00399.
MLA [1] Chengqian Huang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00399.
APA [1] Chengqian Huang, Mengfan Zhu, & Yu Mao. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00399
IEEE [1] Chengqian Huang, Mengfan Zhu, and Yu Mao, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00399. keywords: {grafting;vapor deposition;underwater superoleophobicity;oil−water separation;high flux}