Tracking the Dynamics of a Ag-MnOx Oxygen Reduction Catalyst Using In Situ and Operando X-ray Absorption Near-Edge Spectroscopy AITranslate

Stanford University; Stanford University; Stanford University; Stanford University; Stanford University; Stanford University; Stanford University; Stanford University; SLAC National Accelerator Laboratory; SLAC National Accelerator Laboratory; SLAC National Accelerator Laboratory; Stanford University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Sustainable electricity generation via hydrogen fuel cells requires the development of efficient oxygen reduction reaction (ORR) catalysts. In situ/operando experiments are necessary to uncover the extent of dynamic material changes during catalysis. Herein, we use in situ/operando X-ray absorption near-edge spectroscopy to track Mn valence changes of a promising, ultrathin, porous MnOx layer on a Ag thin film. Mn–K-edge measurements as a function of electrochemical environment and ORR conditions reveal that, interestingly, when driving the ORR at 0.8 VRHE, the Mn is distinctively more reduced and the MnOx redox is nonreversible in contrast to measurements in N2-saturated electrolyte. Ex situ inductively coupled plasma mass spectrometry, atomic force microscopy, and X-ray photoelectron spectroscopy indicate that these phenomena do not correlate to metal dissolution but might be associated with morphological surface reconstruction related to Ag valency. This study highlights how the microenvironment and catalysis play a key role in the in situ/operando surface structure and chemical state.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00823

Chinese Library Classification Number:

Citation Information:

Sustainable electricity generation via hydrogen fuel cells requires the development of efficient oxygen reduction reaction (ORR) catalysts. In situ/operando experiments are necessary to uncover the extent of dynamic material changes during catalysis. Herein, we use in situ/operando X-ray absorption near-edge spectroscopy to track Mn valence changes of a promising, ultrathin, porous MnOx layer on a Ag thin film. Mn–K-edge measurements as a function of electrochemical environment and ORR conditions reveal that, interestingly, when driving the ORR at 0.8 VRHE, the Mn is distinctively more reduced and the MnOx redox is nonreversible in contrast to measurements in N2-saturated electrolyte. Ex situ inductively coupled plasma mass spectrometry, atomic force microscopy, and X-ray photoelectron spectroscopy indicate that these phenomena do not correlate to metal dissolution but might be associated with morphological surface reconstruction related to Ag valency. This study highlights how the microenvironment and catalysis play a key role in the in situ/operando surface structure and chemical state.

quote

GB/T 7714-2015 [1] Johanna Schröder, José A. Zamora Zeledón, Gaurav A. Kamat, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00823.
MLA [1] Johanna Schröder, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00823.
APA [1] Johanna Schröder, José A. Zamora Zeledón, Gaurav A. Kamat, Melissa E. Kreider, Lingze Wei, Aniket S. Mule, Armando Torres, Kyra Yap, Dimosthenis Sokaras, Alessandro Gallo, Michaela Burke Stevens, & Thomas F. Jaramillo. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00823
IEEE [1] Johanna Schröder, José A. Zamora Zeledón, Gaurav A. Kamat, Melissa E. Kreider, Lingze Wei, Aniket S. Mule, Armando Torres, Kyra Yap, Dimosthenis Sokaras, Alessandro Gallo, Michaela Burke Stevens, and Thomas F. Jaramillo, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00823.