High-Energy-Density, Long-Life Li-Metal Batteries via Application of External Pressure AITranslate
Abstract AITranslate
The application of commercially available carbonate-based electrolytes to Li-metal batteries (LMBs) is challenging because of the uncontrollable side reactions of the electrolytes with Li anodes. Herein, a practical carbonate-electrolyte-based LMB with a high areal capacity and long cycle life is proposed. The cycling stability of the proposed LMB is established by applying an external compressive pressure (1200 kPa) and a boehmite-coated separator to prevent the short circuit of the electrodes. The external pressure drives the growth of the Li metal as a dense uniform layer instead of dendrites and mitigates the formation of microcracks in the charged Ni-rich layered cathode. The unprecedented cycling stability of the stacked LMB with a Ni-rich layered cathode, retaining 82.0% of its initial capacity after 500 cycles, can prove instrumental in realizing practical high-energy-density LMBs, thus demonstrating the possibility of employing cell compression to increase the life and energy density of LMBs.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.3c00910
Chinese Library Classification Number:
Citation Information:
The application of commercially available carbonate-based electrolytes to Li-metal batteries (LMBs) is challenging because of the uncontrollable side reactions of the electrolytes with Li anodes. Herein, a practical carbonate-electrolyte-based LMB with a high areal capacity and long cycle life is proposed. The cycling stability of the proposed LMB is established by applying an external compressive pressure (1200 kPa) and a boehmite-coated separator to prevent the short circuit of the electrodes. The external pressure drives the growth of the Li metal as a dense uniform layer instead of dendrites and mitigates the formation of microcracks in the charged Ni-rich layered cathode. The unprecedented cycling stability of the stacked LMB with a Ni-rich layered cathode, retaining 82.0% of its initial capacity after 500 cycles, can prove instrumental in realizing practical high-energy-density LMBs, thus demonstrating the possibility of employing cell compression to increase the life and energy density of LMBs.
quote
| GB/T 7714-2015 | [1] Hun Kim, SuHyun Lee, JaeMin Kim, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00910. |
| MLA | [1] Hun Kim, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00910. |
| APA | [1] Hun Kim, SuHyun Lee, JaeMin Kim, Chong Seung Yoon, & YangKook Sun. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00910 |
| IEEE | [1] Hun Kim, SuHyun Lee, JaeMin Kim, Chong Seung Yoon, and YangKook Sun, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00910. |